| 基于动态相变的热轧C-Mn-Al-Si系TRIP钢组织演变 |
| 尹云洋;杨王王月;李龙飞;杨王玥;孙祖庆;王西涛 |
| 北京科技大学材料科学与工程学院 |
|
| Study on Microstructure Evaluation of hot rolled C-Mn-Si-Al TRIP steel based on dynamic transformation of undercooled austentie |
| ;;;; |
| 北京科技大学 |
引用本文:
尹云洋; 杨王王月; 李龙飞; 杨王玥; 孙祖庆; 王西涛 . 基于动态相变的热轧C-Mn-Al-Si系TRIP钢组织演变[J]. 金属学报, 2008, 44(6): 686-692 .
[1]Ushilda K.Scand J Metall,1999,28:33 [2]Tosal Martinez L,Vanderschueren D,Jacobs S,Van dcputte S.Steel Res,2001;72:412 [3]Bcllhouse E M,Mertens A I M,McDermid J R.Mater Sc Eng,2007;A463:147 [4]Pichlcr A,Stiaszny P.Steel Res,1999;70:457 [5]Girault E,Mcrtens A,Jacques P,Houbaert Y,Verlinden B,Van Humbeeck J.Scr Mater,2001;44:885 [6]Barbe L,Verbeken K,Wettinck E.ISIJ lnt,2006;46:1251 [7]Meyer D,Vanderschueren D,De Cooman B C.ISIJ lnt 1999;39:813 [8]Jacques P J,Girault E,Mertens A,Verlinder B,Van Hum beeck J,Delannay F.ISIJ lnt,2001;41:1068 [9]Basuki A,Aernoudt E.Scr Mater,1999;40:1003 [10]Timokhina I B,Hodgson P D,Pereloma E V.Metall Mate Trans,2003;34A:1599 [11]Ryu H B,Speer J G,Wise J P.Metall Mater Trans,2002 33A:2811 [12]Yang W Y,Qi J J,Sun Z Q,Yang P.Acta Metall Sin 2004;40:135 (杨王玥,齐俊杰,孙祖庆,杨平.金属学报,2004:40:135) [13]Yang P,Fu Y Y,Cui F E,Sun Z Q.Acta Mctall Sin,2001; 37:592 (杨平,傅云义,崔凤娥,孙祖庆.金属学报.2001:37:592) [14]Mahieu J,Maki J,De Cooman B C,Claessens S.Metall Mater Trans,2002;33A:2573 [15]Mintz B.lnt Mater Rev,2001;46:169 [16]Miller R L,Trans ASM,1964;57:892 [17]Sung-Joon K,Chang G L,Ildong C,Sunghak L.Metall Mater Trans,2001;32A:505 [18]Qi J J,Yang W Y,Sun Z Q,Zhang X Z,Dong Z F.Acta Metall Sin,2005;41:605 (齐俊杰,杨王玥,孙祖庆,章晓中,董志峰.金属学报,2005;41:605) [19]De Meyer M,Mahicu J,De Cooman B C.Mater Sci Tech- nol,2002;18:1121 [20]Sakuma Y,Matsumura O,Takechi tl.Metall Trans,1991; 22A:489 [21]Lee Y K,Shin tt C,Jang Y C,Kim S H,Choi C S.Set Mater,2002;47:805 [22]Bhadeshia H K D H,Waugh A R.Aeta Metall,1982;30: 775 [23]ttanzaki A Z,Hodgson P D,Yue S.Metall Mater Trans, 1997;28A:2405 [24]Timokhina I B,Hodgson P D,Pcreloma E V.In:De Cooman B C ed.,Proc of Int Conf on TRIP Aided High Strength Ferrous Alloys,Wisscnschafts Vcrlag Mainz GmbH,Aachen,2002:181 [25]Tsuzaki K,Fukasaku S,Tomota Y,Maki T.Mater Trans, JIM,1991;32:222 [26]Singh S B,Bhadeshia H K D H.Mater Sci Technol,1996; 12:610 [27]Shipway P H,Bhadeshia H K D H.Mater Sei Technol, 1995;11:1116 [28]Luo H W,Zhao L,Kruijver S O,Sictsma J,Van der Zwaag S.ISIJ Int,2003;43:1219 [29]Jacques P,Cornet X,Harlot Ph,Ladricre J,Delannay F. Metall Mater Trans.1998;29A:2383 [30]Kawano O,Wakita.J,Esaka K,Abe It.Iron Steel Inst Jpn Int,1996;82:232 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|