| 快速冷却条件下Cu--Co合金的凝固 |
| 赵九洲;李海丽;何杰;张显飞 |
| 金属所 |
|
| Solidification of Cu-Co ally under rapid cooling conditions |
| ;;; |
| 金属所 |
引用本文:
赵九洲; 李海丽; 何杰; 张显飞 . 快速冷却条件下Cu--Co合金的凝固[J]. 金属学报, 2008, 44(6): 693-697 .
,
,
,
.
Solidification of Cu-Co ally under rapid cooling conditions[J]. Acta Metall Sin, 2008, 44(6): 693-697 .
[1]Nakagawa Y.Acta Metall,1958;6:704 [2]Elderrandall S P,Munitz A,Abbaschian R.Mater Sci Fo- rum,1989;50:137 [3]Munitz A,Elderrandall S P,Abbaschian R.Metall Mater Trans,1992;23A:1817 [4]Munitz A,Abbaschian R.Metall Mater Trans,1996;27A: 4049 [5]Munitz A,Abbaschian R.J Mater Sci,1998;33:3639 [6]Yamauchi I,Ueno N,Shimaoka M,Ohnaka I.J Mater Sci, 1998;33:371 [7]Cao C D,Gorler G P,Herlach D M,Wei B.Mater Sci Eng,2002;A325:503 [8]Wilde G,Perepezko J H.Acta Mater,1999;47:3009 [9]Busch R,Gartner F,Borchers C,Haasen P,Bormann R. Acta Metall Mater,1995;43:3467 [10]Li D,Robinson M B,Rathz T J,Williams G.Mater Lett, 1998;36:152 [11]Lu Q Q,Fontaine J R,Aubertin G.lnt J Heat Mass Trans- fer,1993;36:79 [12]Clif R,Grace J R,Weber M E.Bubbles,Drops and Par- ticles.New York:Academic Press,1978:111 [13]Ranz W E,Marshall W R.Chem Eng Prog,1952;48:141 [14]Zhao J Z,Ratke L,Jia J,Li Q C.J Mater Sci Technol, 2002;18:197 [15]Catalina A V,Mukherjee S,Stefanescu D M.Metall Mater Trans,1999;31A:2559 [16]Zhao J Z,Ratke L,Feuerbacher B.Modelling Simul Mater Sci Eng,1998;6:123 [17]Granasy L,Ratke L.Scr Metall Mater,1993;28:1329 [18]Lehtinen K E J,Zachariah M R.J Colliod Interface Sci, 2001;242:314 [19]Zhao J Z,Kolbe M,Li H L,Gao J R,Ratke L.Metall Mater Trans,2007;38A:1162 [20]Falk F.In:Ratke L ed.,Immiscible Metals and Organ- ics,DGM-Informationsgesellschaft,Oberursel,Germany, 1993:93 [21]Nachtrieb H.Adv Phys,1967;16:309 [22]Larsson S J,Roxbergh C,Lodding A.Phys Chem Liq, 1972;3:137 [23]Swalin R A.Acta Metall,1959;7:736 [24]Leak V G,Swalin R A.Trans Metall Soc AIME,1964; 230:426 [25]Swalin R A,Leak V G.Acta Metall,1965;13:471, |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|