中间退火温度对多道次冷轧Al-Mg-Sc-Zr合金力学性能的影响 |
杜刚;闫德胜;戎利建 |
中国科学院金属研究所特殊环境材料研究部 |
|
Influence of intermediate annealing temperature on strength of repeat cold-rolled Al-Mg-Sc-Zr alloy |
Gang Du;Desheng Yan; |
中国科学院金属研究所特殊环境材料研究部 |
引用本文:
杜刚; 闫德胜; 戎利建 . 中间退火温度对多道次冷轧Al-Mg-Sc-Zr合金力学性能的影响[J]. 金属学报, 2008, 44(10): 1209-1212 .
,
,
.
Influence of intermediate annealing temperature on strength of repeat cold-rolled Al-Mg-Sc-Zr alloy[J]. Acta Metall Sin, 2008, 44(10): 1209-1212 .
[1]Tang M J,Ji Z S,Lu X Y.Light Alloy Fabr Technol,2004; 32(7):1 (唐明君,吉泽升.吕新宇.轻合金加工技术,2004;32(7):1) [2]Gabriel M N,Alan J A.Mater Sci Eng,2001;A318:144 [3]Miura Y,Shioyama T,Hara D.Mater Sci Forum,1996; 217-222:505 [4]Dougherty L M,Robertson I M,Vetrano J S.Acta Mater, 2003;51:4367 [5]Ashby M F,Brown L M.Philos Mag,1963;8A:1083 [6]Royset J,Ryum N.Int Mater Rev,2005;50:19 [7]Huang Q Y,Li H K.Superalloy.Beijing:Metallurgical Industry Press,2000:22 (黄乾尧,李汉康.高温合金.北京:冶金工业出版社,2000:22) [8]Shi D K.Dislocation and Strength of Metals.Xi'an:Xi'an Jiaotong University Press,1998:137 (石德科.位错与材料强度西安:西安交通大学出版社,1998:137) [9]Zhao W T,Yan D S,Rong L J.Trans Nonferrous Metals Soc China,2006;16:175 [10]Alan J A.Acta Metall,1967;15:1775 [11]Marquis E A,Seidman D N.Acta Mater,2001;49:1909 [12]Sun Z Y,Liu C M.Diffusion and Phase Transformation in Alloys.Shenyang:Northeastern University Press,2002: 137 (孙振岩,刘春明.合金中的扩散与相变.沈阳:东北大学出版社,2002:137) [13]Pan J S,Tong J M,Tian M B.Foundation of Material Science.Beijing:Tsinghua University Press,1998:465 (潘金生,仝健民,田民波.材料科学基础.北京:清华大学出版社,1998:465) [14]Iwamura S,Miura Y.Acta Mater,2004;52:591 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|