| 马氏体岛的体积分数、形状及强度对粒状组织钢力学性能的影响 |
| 许峰云;白秉哲;方鸿生 |
| 清华大学材料科学与工程系先进材料教育部重点实验室 |
|
| The influence of martensite volume fraction, shape and strength on the mechanical properties of granular structure steels |
| Xu Feng-yun;; |
| 北京清华大学材料科学与工程系 |
引用本文:
许峰云; 白秉哲; 方鸿生 . 马氏体岛的体积分数、形状及强度对粒状组织钢力学性能的影响[J]. 金属学报, 2008, 44(10): 1183-1187 .
,
,
.
The influence of martensite volume fraction, shape and strength on the mechanical properties of granular structure steels[J]. Acta Metall Sin, 2008, 44(10): 1183-1187 .
[1]Jiang Z H,Guan Z Z,Lian J S.J Mater Sci,1993:28: 1814 [2]Davies R G.Metall Trans,1978;9A:451 [3]Goel N C,Tseng D,Tangri K.Scr Metall,1984;18:873 [4]Araki K,Takada Y,Nakaoka K.Trans Iron Steel Inst Jpn, 1977;17:710 [5]Shen X P,Lei T Q.Acta Metall Sin,1984;20:A271 (沈显璞.雷廷权.金属学报,1984;20:A271) [6]Tomota Y,Kuroki K,Mori T,Tamura I.Mater Sci Eng, 1976;24:85 [7]Al-Abbasi F M,Nemse J A.Int J Mech Sci,2003;45: 1449 [8]Al-Abbasi F M,Nemes J A.Int J Solid Struct,2003;40: 3379 [9]Prahl U,Papaefthymiou S,Uthaisangsuk V,Bleck W,Si- etsma J,Zwaag S V D.Comput Mater Sci,2007;39:17 [10]Uthaisangsuk V,Prahl U,Bleck W.Cornput Mater Sci, 2008;43:27 [11]Xia Y M,Zhou Y X,Yang B C.Mater Sci Technol,1997; 5(1):60 (夏源明,周元鑫,杨报昌.材料科学与工艺,1997;5(1):60) [12]Eshelby J D.Proc R Soc London,1957;241A:376 [13]Takao Y,Chou T W,Taya M.J Appl Mech,1982;49:536 [14]Tszeng T C.J Cornp Mater,1994;28:800 [15]Tszeng T C.Comp Sci Technol,1994;51:75 [16]Mori T,Tanaka K.Acta Metall,1973;21:571 [17]Hüper T,Endo S,Ishikawu N,Osawa K.ISIJ Int,1999; 39:288 [18]Chert H C,Cheng G H.J Mater Sci,1989;24:1991 [19]Byun T S,Kim I S.J Mater Sci,1993;28:2923 [20]Shen H P,Lei T C,Liu J Z.Mater Sci Technol,1986;2: 28 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|