| 下贝氏体中碳化物的析出 |
| 方鸿生 冯春 郑燕康 郑秀华 张弛 白秉哲 |
| 清华大学材料科学与工程系先进材料教育部重点实验室; 北京 100084 |
|
| The lower bainitic carbides are precipitated from austenite |
| ;FENG Chun;;;;; |
| 清华大学材料系 |
引用本文:
方鸿生; 冯春; 郑燕康; 郑秀华; 张弛; 白秉哲 . 下贝氏体中碳化物的析出[J]. 金属学报, 2007, 43(6): 583-588 .
,
,
,
,
,
.
The lower bainitic carbides are precipitated from austenite[J]. Acta Metall Sin, 2007, 43(6): 583-588 .
[1]Hehemann R F,Kinsman K R,Aaronson H I.Metall Trans,1972;3:1077 [2]Hsu T Y,Gu W,Yu X.Proc Int Conf Solid-Solid Phase Transform,New York:Metallurgical Society of AIME, 1982:1029 [3]Aaronson H I.Metall Trans,1990;21A:1343 [4]Fang H S,Yang Z G,Yang J B,Bai B Z.Acta Metall Sin, 2005;41:449 (方鸿生,杨志刚,杨金波,白秉哲.金属学报,2005;41:449) [5]Azuma M,Fujita N,Takahashi M.ISIJ Int,2005;45:221 [6]Bhadeshia,H K D H,Edmonds D V.Acta Metall,1980; 28:1265 [7]Bhadeshia H K D H.Acta Metall,1980;28:1103 [8]Bhadeshia H K D H.Bainite in Steels.London:The ??Cambridge University Press,2001:68,70 [9]Kang M K,Sun J L,Yang Q M.Metall Trans,1990;21A: 853 [10]Peet M,Babu S S,Miller M K,Bhadeshia H KD H.Scr Mater,2004;50:1277 [11]Kang M K,Zhang M X,Zhu M.Acta Mater,2006;54: 2121 [12]Honeycombe R W K.In:Marder A R,Goldstein J I eds, Proc Int Conf Phase Transformation in Ferrous Alloys. Warrendale,PA:TSM-AIME,1983:259 [13]Fang H S,Wang J J,Zheng Y K,Yang Z G.Acta Metall Sin,1993;29:445 (方鸿生,王家军,郑燕康,杨志刚.金属学报,1993;29:445) [14]Aaronson H I.Metall Trans,1993;24A:241 [15]Aaronson H I.Journal of Microscopy,1974;102:275 [16]Fang H S,Wang J J,Yang Z G,Li C M,Bo X Z,Zheng Y K.Bainite Transformation.Beijing:Science Press,1999: 64,225,512 (方鸿生,王家军,杨志刚,李春明,薄祥正,郑燕康.贝氏体相变.北京:科学出版社,1999:64,225,512) [17]Fang H S,Bo X Z,Wang J J.Mater Trans JIM,1998;39: 1264 [18]Fang H S,Wang J J,Zheng Y K.Metall Trans,1994;25A: 1 [19]Jin Q,Fang H S.Metall Trans,1990;21A:2637 [20]Xu Z Y.Theory of Phase Transformation.Beijing:Sci- ence Press,1988:366 (徐祖耀.相变原理.北京:科学出版社,1988:366) [21]Fang H S,Wang J J,Yang Z G,Li C M,Zheng Y K. Metall Trans,1996;27A:1535 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|