| 纳米压痕法测量Sn--Ag--Cu无铅钎料BGA焊点的力学性能参数 |
| 王凤江 钱乙余 马 鑫 |
| 哈尔滨工业大学现代焊接生产技术国家重点实验室; 哈尔滨 150001 |
|
| Measurement of Mechanical Properties of Sn--Ag--Cu Bulk Solder BGA Solder Joint Using Nanoindentation |
| WANG Fengjiang; QIAN Yiyu; MA Xin |
| State Key Laboratory of Advanced Welding Production Technology; Harbin Institute of Technology; Harbin 15000 |
引用本文:
王凤江; 钱乙余; 马鑫 . 纳米压痕法测量Sn--Ag--Cu无铅钎料BGA焊点的力学性能参数[J]. 金属学报, 2005, 41(7): 775-779 .
,
,
.
Measurement of Mechanical Properties of Sn--Ag--Cu Bulk Solder BGA Solder Joint Using Nanoindentation[J]. Acta Metall Sin, 2005, 41(7): 775-779 .
[1] Manson S S. Thermal Stress and Low-Cycle Fatigue. New York: Mcgraw-Hill, 1966 [2] Villain J, Brueller O S, Qasim T. Sens Actuators, 2002; 99A: 194 [3] Wiese S, Feustel F, Meusel E. Sens Actuators, 2002; 99A: 188 [4] Wiese S, Schubert A, Walter H, Dudek R, Feustel F, Meusel E, Michel B. In: Proceedings IEEE 51th Electronic Components and Technology Conference, Orlando: IEEE, 2001: 890 [5] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564 [6] Suresh S, Giannakopoulos A E. Acta Mater, 1998; 46: 5755 [7] Giannakopoulos A E, Suresh S. Scr Mater, 1999; 40: 1191 [8] Fujiwara M, Otsuka M. Mater Sci Eng, 2001; A319-321: 929 [9] Ma X, Yoshida F. Appl Phys Lett, 2003; 82: 188 [10] Zeng K, Tu K N. Mater Sci Eng Rep, 2002; 38: 55 [11] JIS Z 3198. Test Methods for Lead-Free Solders, Japanese Industrial Standard, 2003 [12] Stiwell N A, Tabor D. Prog Phys Soc, 1961; 78: 169 [13] Johnson K L. J Mech Phys Solids, 1970; 18: 115 [14] Pao Y H, Badgley S, Govila R, Jih E. Mater Res Soc Symp Proc, 1994; 323: 128 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|