| 可调拘束实验测量的焊接凝固裂纹阻力曲线的有限元法修正 |
| 董志波 魏艳红 刘仁培 |
| 哈尔滨工业大学现代焊接生产技术国家重点实验室; 哈尔滨 150001 |
|
| Fem Modifying the Resistance Curve of Weld Metal Solidification Crack Measured by Trans-Varestraint Test |
| DONG Zhibo; WEI Yanhong; LIU Renpei |
| State Key Laboratory of Advanced Welding Technology Production; Harbin Institute of Technology; Harbin 150001 |
引用本文:
董志波; 魏艳红; 刘仁培 . 可调拘束实验测量的焊接凝固裂纹阻力曲线的有限元法修正[J]. 金属学报, 2005, 41(7): 780-784 .
,
,
.
Fem Modifying the Resistance Curve of Weld Metal Solidification Crack Measured by Trans-Varestraint Test[J]. Acta Metall Sin, 2005, 41(7): 780-784 .
[1] Feng Z L. PhD Dissertation, Ohio State University, Ohio, 1993 [2] Savage W F, Lundin C D. Weld J, 1965; 10: 433 [3] Senda T, Matsuda F. Trans Jpn Weld Soc, 1971; 2(2):1 [4] Arata Y, Matsuda F. Trans JWRI, 1976; 5(21): 53 [5] Matsuda F, Arata Y. Trans JWRI, 1977; 6(21): 197 [6] Matsuda F, Nakagawa H. Trans JWRI, 1983; 12(1):65 [7] Wei Y H, Liu R P, Dong Z Z. Chin Weld, 2000, 9(1): 36 [8] Goldak J. Metall Trans, 1984; 15B: 587 |
|