| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang110016 |
引用本文:
杨义; 徐锋; 黄爱军; 李阁平 . 全片层BT18Y钛合金在相区固溶时的显微组织演化[J]. 金属学报, 2005, 41(7): 713-720 .
,
,
,
.
Evolution of Microstructure of Full Lamellar Titanium Alloy BT18Y Solutionized At Phase Field[J]. Acta Metall Sin, 2005, 41(7): 713-720 .
[1]Lee D H,Nam S W.Scr Mater,1999;40:265 [2]Bolisowa E A.Translated by Chen S Q.Metallography of Titanium Alloys.Beijing:Defense Industrial Press,1980: 246,214,227,199 (鲍利索娃E.A.编著,陈石卿译.钛合金金相学.北京:国防 工业出版社,1986:246,214,227,199) [3] Wang Q Y,Ge Z M,Zhou Y B.Aerial Titanium Alloy. Shanghai:Shanghai Science and Technology Press,1985: 209,211,302 (王全友,葛志明,周彦邦.航空用钛合金.上海:上海科学技 术出版社, 1985:210,190,302) [4]Filip R,Kubiak K,Ziaja W,Sieniawski J.Mater Proc Technol,2003;133:84 [5]Peng C Q,Huang B Y,He Y H.Chin Nonferrous Met, 2001;11:527 (彭超群,黄伯云,贺跃辉.中国有色金属学报,2001;11:527) [6] Tiley J,Searles T,Lee E,Kar S,Banerjee R,Russ J C, Fraser H L.Mater Sci Eng,2004;A372:191 [7] Lee D H, Nam S W, Choe S J. Mater Sci Eng, 2000; A291: 60 [8] Semiatin S L, Seetharaman V, Ghosh A K, Shell E B, Simon M P, Fagin P N. Mater Sci Eng, 1998; A256: 92 [9] Seshacharyulu T, Medeiros S C, Morgan J T, Malas J C, Frazier W G, Prasad Y V R K. Mater Sci Eng, 2000; A279: 289 [10] Seshacharyulu T, Medeiros S C, Frazier W G, Prasad Y V R K. Mater Sci Eng, 2002; A325: 112 [11] Sauer C, Lutjering G.Mater Sci Eng, 2001; A319-321: 393 [12] Lutjering G. Mater Sci. Eng, 1999; A263: 117 [13] Zhang X D, Bonniwell P, Fraser H L, Baeslack W A, Evans D J, Ginter T, Bayha T, Cornell B. Mater Sci Eng, 2003; A343: 210 [14] Koike J, Maruyama K. Mater Sci Eng, 1999; A263: 155 [15] Furuhara T, Ogawa T, Maki T. Philos Mag Lett, 1995; 72 (3): 175 [16] Bhattacharyya D, Viswanathan G B, Robb D, Furrer D, Hamish L F. Acta Mater, 2003; 51: 4679 [17] Huang A J, Xu F, Li G P, Li D. Acta Metall Sin, 2002; 38(Suppl.): S217 (黄爱军,徐锋,李阁平,李 东.金属学报, 2002;3s(增 刊):S217) [18] Furuhara T, Takagi S, Watanabe H, Maki T. Metall Trans, 1996; 27A: 1635 [19] Miyano N, Fujiwara H, Ameyama K, Weatherly G C. Mater Sci Eng, 2002; A333: 85 [20] Cui Z Q. Metallography and Heat Treatment. Beijing: China Machine Press, 1995: 257 (崔忠圻.金属学与热处理.北京:机械工业出版社,1995:257) [21] Xia L F. Metallic Heat Treatment Technology. Herbin: Harbin University of Technology Press, 1998: 28 (夏立芳.金属热处理工艺学.哈尔滨:哈尔滨工业大学出版社, 1998:28) [22] Xu Z Y. The Theory of Phase Transition. Beijing: Science Press, 2000: 22 (徐祖耀.相变原理.北京:科学出版社, 2000:22) [23] Huang A J, Li G P, Hao Y L,Yang R. Ada Mater, 2003; 51: 4939 [24] Viswanathan G B, Karthikeyan S, Hayes R W, Mills M J. Acta Mater, 2002; 50: 4965 [25] Savage M F, Tatalovich J, Zupan M, Hemker K J, Mills M J. Mater Sci Eng, 2001; A319-321: 398 [26] Seward G G E, Celotto S, Prior D J, Wheeler J, Pond R G. Acta Mater, 2004; 52: 821H |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|