| 不锈钢在循环扭转载荷下近门槛值的疲劳裂纹扩展行为 |
| 于慧臣 张岩基 孙燕国 谢世殊 田中启介 |
| 北京航空材料研究院; 北京 100095 |
|
| Near Threshold Fatigue Crack Growth Behavior in Stainless Steel |
| YU Huichen;ZHANG Yanji; SUN Yanguo; XIE Shishu; TANAKA Keisuke |
| Beijing Institute of Aeronautical Materials; Beijing 100095 |
引用本文:
于慧臣; 张岩基; 孙燕国; 谢世殊; 田中启介 . 不锈钢在循环扭转载荷下近门槛值的疲劳裂纹扩展行为[J]. 金属学报, 2005, 41(7): 721-726 .
,
,
,
,
.
Near Threshold Fatigue Crack Growth Behavior in Stainless Steel[J]. Acta Metall Sin, 2005, 41(7): 721-726 .
[1] Pook L P. Int J Fatigue, 1985; 7(1): 21 [2] Yates J R, Miller K J. Fatigue Fract Eng Mater Struct, 1989; 12: 259 [3] Yoshioka S, Watanabe K, Kitagawa H, Inoue A, Kumar sawa M. Trans Jpn Sod Mech Eng, 1984; 50(453): 1267 [4] Tschegg E K. Mater Sci Eng, 1982; 54: 127 [5] Tschegg E K. J Mater Sci, 1983; 18: 1604 [6] Yu H C, Tanaka K, Akiniwa Y. Fatigue Fract Eng Mater Struct, 1998; 21: 1067 [7] Yu H C, Xie S S, Tanaka K, Akiniwa Y. J Mater Eng, 2002; (Suppl.): 317 (于慧臣,谢世殊,田中启介,秋庭义明.材料工程,2002;(增 刊):317) [8] Yu H C, Xie S S, Sun Y G, Tanaka K. J Aeronaut Mater, 2004; 24(5): 53 (于慧臣,谢世殊,孙燕国,田中启介.航空材料学报, 2004; 24(5):53) [9] Yu H C, Sun Y G, Xie S S, Tanaka K. Acta Metall Sin, 2005; 41: 73 (于慧臣,孙燕国,谢世殊,田中启介.金属学报, 2005;41: 73) [10] Ritchie R O, McClintock F A, Hayeb-Hashemi H, Ritter M A. Metall Trans, 1982; 13A: 101 [11] Tada H, Paris P C, Irwin G R. The Stress Intensity Factor Handbook. 2nd ed., 1985: 27 [12] Tanaka K, Akiniwa Y, Nakamura H. Fatigue Fract Eng Mater Struct, 1996; 19: 571 [13] Tanaka K, Akiniwa Y, Yu H C. ASTM STP 1359, 1999: 295 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|