| Ni52Mn21+xGa27-x(x=0—5)磁性形状记忆合金的相变 |
| 郭世海 张羊换 李健靓 祁焱 王新林 |
| 郭世海(钢铁研究总院功能材料所; 北京 100081 |
|
| Phase Transformation in Ni52Mn21+xGa27-x(x =0-5) Magnetic Shape Memory Alloys |
| GUO Shihai; ZHANG Yanghuan; LI Jianliang; QI Yan; WANG Xinlin |
| Department of Functional Material Research; Central Iron and Steel Research Institute; Beijing 100081 |
引用本文:
郭世海; 张羊换; 李健靓; 祁焱; 王新林 . Ni52Mn21+xGa27-x(x=0—5)磁性形状记忆合金的相变[J]. 金属学报, 2004, 40(9): 972-974 .
,
,
,
,
.
Phase Transformation in Ni52Mn21+xGa27-x(x =0-5) Magnetic Shape Memory Alloys[J]. Acta Metall Sin, 2004, 40(9): 972-974 .
[1] Ullakko K, Huang J K, Kantner C, O'Handley R C. Appl Phys Lett, 1996; 69: 1966 [2] Murray S J, Hayashi R, Marioni M, Allen S M, O'Handley R C. In: Wuttig M ed., Smart Structures and Materials 1999: Smart Materials Technologies, Newport Beach, CA: The Society of Photo-Optical Instrumentation Engineers (SPIE), 3675, 1999: 204 [3] Schlagel D L, Wu Y L, Zhang W, Lograsso T A. J Alloys Compd, 2000; 312: 77 [4] Henry C P, Bono D, Feuchtwanger J, Allen S M, O'Handley R C. J Appl Phys, 2002; 91: 7810 [5] Ezera Y, Sozinov A, Kimmel G, Etelaniemi V, Glavatskaya N I, D'Anci A, Podgursky V, Lindroos V K, Ullakko K. In: Wuttig M ed., Smart Structures and Materials 1999: Smart Materials Technologies, Newport Beach, GA: The Society of Photo-Optical Instrumentation Engineers (SPIE), 3675, 1999: 244 [6] Webster P J. Philos Mag, 1984; 49B: 295 [7] Wang W H, Wu G H, Chen J L, Yu C H, Gao S X, Zhan W S. J Phys Lett, 2000; 11: 3245 [8] Sozinov A, Likhachev A A, Ullakko K. IEEE Trans Magn, 2002; 38: 2814 [9] Murakami Y, Shindo D, Suzuki M, Ohtsuka M, Itagaki K.Acta Mater, 2003; 51: 485 [10] Ma Y Q, Jiang C B, Feng G, Xu H B. Scr Mater, 2003;48: 365 [11] Vasil'ev A, Bozhko A, Khovailo V, Dikshtein I, Shavrov V, Seletskii S, Buchelnikov V. J Magn Magn Mater, 1999; 197: 837 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|