Zn-Cu包晶合金定向凝固组织演化 I. 实验现象及分析 |
王猛; 林鑫; 苏云鹏; 沈淑娟; 黄卫东 |
西北工业大学凝固技术国家重点实验室; 西安 710072 |
|
引用本文:
王猛; 林鑫; 苏云鹏; 沈淑娟; 黄卫东 . Zn-Cu包晶合金定向凝固组织演化 I. 实验现象及分析[J]. 金属学报, 2003, 39(8): 831-837 .
[1] Kerr H W, Kurz W. Int Mater Rev, 1996; 4: 41 [2] Boettinger W J, Coriell S R, Greer A L, Karma A, KurzW, Rappaz M, Trivedi R. Acta Mater, 2000; 48: 43 [3] Caroli B, Caroli C, Roulet B. Acta Metall, 34, 1986; 34:1867 [4] Hillert M. Solidification and Casting of Metals. London:The Metals Society, 1979: 242 [5] Umeda T, Okane T, Kurz W. Acta Mater, 1996; 44: 4209 [6] Vandyoussefi M, Kerr H W, Kurz W. In: Beech J, JonesH eds., Proc 4th Int Conf on Solidification Processing.Sheffield: The University of Sheffield, 1997: 564 [7] Wang M, Lin X, Su Y P, Shen S J, Huang W D. ActaMetall Sin, 2002; 38: 337(王猛,林鑫,苏云鹏,沈淑娟,黄卫东,金属学报,2002;38:337) [8] Huang W D, Lin X, Wang M, Shen S J, Su Y P, Liu Z X.Sci Chin, 2002; 45E: 458 [9] Aziz M J, Kaplan T. Acta Metall, 1988; 36: 2335n |
|