|
|
|
| Zn-Cu包晶合金定向凝固组织演化 II. 相选择的改进分析 |
| 王猛; 林鑫; 苏云鹏; 沈淑娟; 黄卫东 |
| 西北工业大学凝固技术国家重点实验室; 西安 710072 |
|
引用本文:
王猛; 林鑫; 苏云鹏; 沈淑娟; 黄卫东 . Zn-Cu包晶合金定向凝固组织演化 II. 相选择的改进分析[J]. 金属学报, 2003, 39(8): 838-842 .
[1] Boettinger W J, Coriell S R, Greer A L, Karma A, KurzW, Rappaz M, Trivedi R. Acta Mater, 2000; 48: 43 [2] Kubin L P, Estrin Y. Acta Metall, 1985; 33: 397 [3] Caroli B, Caroli C, Roulet B. Acta Metall, 1986; 34: 1867 [4] Fredriksson H. Metals Handbook. OH: ASM, Metals Park,1988; 15: 125 [5] Gill S C, Kurz W. Acta Metall Mater, 1995; 43: 139 [6] Umeda T, Okane T, Kurz W. Acta Mater, 1996; 44: 4209 [7] Vandyoussefi M, Kerr H W, Kurz W. In: Beech J, JonesH eds., Proc 4th Int Conf on Solidification Processing.Sheffield: The University of Sheffield, 1997: 564 [8] Huang W D, Lin X, Wang M, Shen S J, Su Y P, Liu Z X.Sci Chin E, 2002; 45: 458 [9] Hunziker O, Vandyoussefi M, Kurz W. Acta Mater, 1998;46: 6325 [10] Hunt J D. Mater Sci Eng, 1984; 65: 75 [11] Christian J W. The Theory of Transformations in Metalsand Alloys, Oxford, Pergamon, 1975: 450 [12] Ma D, Li Y, NG S C, Jones H. Acta Mater, 2000; 48: 419 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|