| ZnCl2蒸汽对纯Ni高温氧化的影响 |
| 马海涛; 王来 |
| 大连理工大学材料工程系; 大连 116024 |
|
引用本文:
马海涛; 王来 . ZnCl2蒸汽对纯Ni高温氧化的影响[J]. 金属学报, 2003, 39(6): 644-648 .
[1] Li Y S, Niu Y, Wu W T. Corr Sci Prot Technol, 2000; 12: 224(李远士,牛焱,吴维(山文).腐蚀科学与防护技术,2000;12:224) [2] Spiegel M. Mater Corr, 1999; 50: 373 [3] Kawahara Y. Corr Sci, 2002; 44: 223 [4] Jegede A, Vasantasree V, Hocking M G. J Mater Sci Lett, 1995; 14: 1089 [5] Jegede A, Vasantasree V, Hocking M G. J Mater Sci Lett, 1995; 14: 858 [6] Yao Z, Marek M. Mater Sci Eng A, 1995; 192-193: 994 [7] Li Y S, Wang F G, Niu Y, Wu W T. Rare Met Mater Eng, 2001; 30: 376(李远士,王富岗,牛焱,吴维(山文).稀有金属材料与工程,2001;30:376) [8] Lee Y Y, McNallan M J. Metall Trans A, 1987; 18A(7) : 1099 [9] Shu Y H, Wang F H, Wu W T. Oxid Met, 1999; 52(5/6) : 463 [10] Sato Y, Young D J. Oxid Met, 2001; 55(3/4) : 243 [11] Jacobson N S. Oxid Met, 1986; 26: 157 [12] Spiegel M, Brabke H J. Mater Corr, 1995; 46: 121 [13] Hossain M K, Saunders S R J. Oxid Met, 1978; 12: 1 [14] Shinata Y, Hara M, Nakagawa T. JIM, 1991; 32: 969 [15] Ma H T, Wang L, Li Y S. J Mater Sci Technol, 2003; 19(5) , to be accepted [16] Kanahara Y. Mater High Temp, 1997; 14: 261 [17] Kubaschewki O, Alcock C B. Metallugical Thermochemistry. 5th ed, Oxford, Pergamon Press, 1979: 377 [18] Sato Y, Hara M, Shinata Y. J Jpn Inst Met, 1996; 60: 192 [19] McNallan M J, Liang W W, Kim S H, Kang C T. In: Rapp R A ed, High Temperature Corrosion, NACE, Houston, Tex, USA, 1983: 316 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|