| 高速冲击下钢板的微观组织及绝热剪切带 |
| 段占强 程国强 李守新 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室 110016 |
|
引用本文:
段占强; 程国强; 李守新 . 高速冲击下钢板的微观组织及绝热剪切带[J]. 金属学报, 2003, 39(5): 486-491 .
[1] Zener C, Hollomon J H. J Appl Phys, 1944; 15: 22 [2] Bai Y L, J Mech Phys Solids, 1982; 30: 195 [3] Cho K., Lee S, Nutt S R, Duffy J. Acta Metall Mater, 1993; 41: 923 [4] Wittman C. L., Meyers M A, Park H R. Metall Trans, 1990; 21: 707 [5] Wingrove A L. Metall Trans, 1973; 4: 1829 [6] Meyers M A, Park H R. Acta Metall, 1986; 34: 2493 [7] Lee C G, Park W J, Lee S, Shin K S. Metall Mater Trans, 1998; 29: 477 [8] Bai Y L. Res Mech, 1990, 31: 133 [9] Shwaki T G. J Appl Mech (Trans ASME), 1994; 61: 538 [10] Dai L. Ling H, Z, Bai Y L. Key Eng Mater, 2000; 177: 401 |
|