| 950℃长期时效对Ni3Al基合金IC6的组织及力学性能的影响 |
| 宋尽霞 肖程波 李树索 韩雅芳 |
| 北京航空材料研究院.北京100095 |
|
引用本文:
宋尽霞; 肖程波; 李树索; 韩雅芳 . 950℃长期时效对Ni3Al基合金IC6的组织及力学性能的影响[J]. 金属学报, 2002, 38(3): 250-254 .
[1] Han Y F, Xing Z P, Chaturvedi M C. In: Nathal M V,Darolia R, Liu C T, Martin P L, Miracle D B, Wagner R,Yamaguchi M ed. Structural Intermetallics 1997,Penn-sylvania:TMS, 1997:713 [2]Fuchs G E, In: Fuchs G E, Dannemann K A, Deragon T Ceds., Long Term Stability of High Temperature Materials,Pennsylvania: TMS, 1999:3 [3]Janowski G M, Harmon B S, Pletka B. J Met Trans, 1987;18A:1341 [4]Pollock T M. Mater Sci Eng, 1995; 32B:255 [5]Murata Y. J Mater Sci, 1983; 23:2069 [6]Tawancy H M. J Mat Sci, 1981; 16:2883 [7]Garossen T J, McCathy G P. Metall Trans, 1985;16A:1213 [8]Liu W C, Chen Z L, Yao M. Metall Trans, 1999; 30A:31 [9]Han Y F, Li S H, Jin Y, Chaturvedi M C. Mater Sci Eng,1985; 192/193A:899 [10]Xiao C B, Wang B L, Li S S, Han Y F. Mater Eng(Suppl),2001:1(肖程波,王蓓蕾,李树索,韩雅芳.材料工程.2001增刊:1) [11]Wang B L, Han Y F, Liao H. Mater Eng, 2000; 3: 11(王蓓蕾,韩雅芳,廖 辉.材料工程,2000;3:11) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|