镶嵌晶粒和晶界对铜双晶体循环变形行为的影响 |
张哲峰 胡运明 王中光 |
中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳 110015 |
|
引用本文:
张哲峰; 胡运明; 王中光 . 镶嵌晶粒和晶界对铜双晶体循环变形行为的影响[J]. 金属学报, 1999, 35(7): 715-720 .
[1]Mughrabi H.Mater Sci Eng,1978;33:207 [2] Cheng A S,Laird C Mater Sci Eng,1981;51:111 [3] Laird C, Charsley P, Mughrabi H. Mater, Sci Eng, 1986;86: 433 [4]Chuang Y-D,Margolin H.Metall Trans,1973;4A:1905 [5] Rey C, Zaoui A. Acta Metall, 1982 30: 523 [6] Peralta P, Laird C. Acta Mater, 1997;45: 3029 [7] Hu Y M; Wang Z G.Mater Sci Eng; 1996; A208: 260 [8] Hu Y M, Wang Z G Acta Mateer 1997; 45: 2655 [9] Zhang Z F, Wang Z G Acta Mateer,1998; 46: 5063 [10] Zhang Z F, Wang Z G. Philos Mag Lett, 1998 78: 105 [11]Gong B,Chen D L,Wang R,Wang Z G.Scr Mater,1997; 37:1605 [12] Li X W, Hu Y M, Wang Z G. Mater Sci Eng, 1998; A248: 299* |
|