| NiAl-28Cr-5Mo-1Hf多相金属间化合物的显微组织及力学性能研究 |
| 崔传勇 郭建亭 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
崔传勇; 郭建亭 . NiAl-28Cr-5Mo-1Hf多相金属间化合物的显微组织及力学性能研究[J]. 金属学报, 1999, 35(5): 477-481 .
[1] Darolia R, Walston U' S, Nathal M V. In: Kissinger H D,Beye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M,Woodford D A eds, Superulloys 1996. Warrendale, Pennsyl-vania: The Minerals,Metals,Materials Society, 1996: 561 [2] Guha S, Munroe P R, Baker I. Mater Sol Egg, 1991, 131A : 27 [3] Darolia R, Lahrman D, Field R D. Scr Metall Mater, 1992;26: 1007 [4] Chen X F, Johnson D R, Oliver B F. Scs Metall Mater, 1994;30: 975 [5] Chen X F, Johnson D R, Noebe R D, Oliver B F. J MaterRes, 1995; 10: 1159 [6] Johnson D R, Chen X F, Oliver F, Noebe R D. Whitteu-berger J D. Intermet,1995; 3: 99 [7] Darolia R. JOM, 1991; 43: 44 [8] Darolia R. In: Darolia R, Noebe R D, Whittenberger J Deds, International Symposium on Structural Intermetallics,Warrendale PA:The Minerals, Metals and Materials Society,1993: 495 [9] Jiang D T, Guo J T. bated Lett, 1998, 36. 33 [10] Jiang D T, Guo J T. Mater Set Egg, 1998; 255A: 154 [11] Whittenberger J D. J Mater Sol, 1987, 22. 394 [12] Zeumer B, Wunnike-Sanders W, Sauthoff G. Mater Sci Eng,1995; (192/193)A: 817 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|