| GTAW外加间歇交变纵向磁场的数值计算及其对焊接行为的影响 |
| 罗键 贾涛 殷咸青 贾昌申 薛锦 |
| 西安交通大学焊接研究所; 西安 710049 |
|
引用本文:
罗键; 贾涛; 殷咸青; 贾昌申; 薛锦 . GTAW外加间歇交变纵向磁场的数值计算及其对焊接行为的影响[J]. 金属学报, 1999, 35(3): 330-333 .
[1] Jia C S, Yin X Q. i Xi'an Jiaotong Univ, 1994; 28: 7(贾昌申,殷咸青.西安交通大学学报,1994;28:7) [2] Malinowski M, Ouden G, Vink P W J. Weld Res, 1990:2(Suppl): 52 [3] Villafuerte J C, Kerr H W. Weld Res, 1990; 2(Suppl): 1 [4] Lei Y Z, Li Q F. J Xi'an Jiaotong Univ, 1989; 23(Suppl.1):109(雷银照,励庆孚.西安交通大学学报,1989,23(增1):109) [5] Selyanenkov V N. Weld Produc, 1975; 22. 50 [6] Abralov M A, abdurak R U, Iuldashev A T. Autom Weld,1977; 30: 52 [7] Matsuda F. Trans JWRI, 1978; 7. 1110 |
|