铸造镍基高温合金中的初生μ相 |
郑运荣 |
北京航空材料研究院; 北京 100095 |
|
引用本文:
郑运荣 . 铸造镍基高温合金中的初生μ相[J]. 金属学报, 1999, 35(12): 1242-1245 .
[1] Zheng Y R, Cat Y L. In: Special Issue of Aeronautical Materials (1), 1977: 5(郑运荣、蔡玉林见:航空材料专集(1),1977:5) [2] Walston W S, O'Hara K S, Ross E W, Pollock T M, MurphyW H. In: Kissinger R D, Deby D J, Anton D L, Cetel A D,Nathal M V, Pollck T M, Woodford D A eds., Soptralloys1996 Warrendale, Pennsylvania: TMS, 1996: 27 [3] Cat Y L, Zheng Y R. Acta Metall Sin, 1982; 18: 30(蔡玉林、郑运荣.金属学报,1982;18:30) [4] Pessah M, Caron P, Khan T. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klastrom D L eds., Superalloys 1992. Warrendale, Pennsylvanie:TMS, 1992: 567 [5] Donachie M J, Krieg O H. J Mater, 197.2; 7: 269 |
|