激光熔覆多元复合硬质合金覆层中颗粒相的行为特征 |
王忠柯 郑启光 陶曾毅 叶和清 陈清明 |
华中理工大学激光技术国家重点实验室; 武汉 430074 |
|
引用本文:
王忠柯; 郑启光; 陶曾毅; 叶和清; 陈清明 . 激光熔覆多元复合硬质合金覆层中颗粒相的行为特征[J]. 金属学报, 1999, 35(10): 1027-1030 .
[1] An S M, Met Y. Acta Metall Sin, 1996;32: 382(安世民,梅雨.金属学报,1996; 32:382) [2] Ariely S,Bamberger M,HogelH,Schoef P.J Mate,Sci,1995; 30:1849 [3] Pei Y T, Meny Q C Ouyans J H Let T Q Chin J Laser,1995; A22:93 (裴字韬,孟庆昌,欧阳家虎,雷廷权、中国激光, 1995; A22: 936) [4] Let T Q, Ouyang J H, Pei Y T, Zhou Y Mater Sci Technol, 1995;11:520 [5] Zeng X Y, Wu X W, Tao Z Y, Zhu B D, Cui K. Acta Metall Sin;1997; 33:885 (曾晓雁,吴新伟,陶曾毅,朱蓓蒂,崔.金属学报,199 33:885) [6]Wu X W, Zeng X Y, Zhu B D, Tao Z Y, CuI K Acta Metall Sin,1997; 33:1282 (吴新伟,曾晓雁,朱蓓蒂,陶曾毅,崔,金属学报,1997: 33:1282) [7] Cooper K P, Ayers J D.J Vac Sci Technol, 1986; 4A: 285 [8] Fang J,Zheng Q G,Wang T,Tao X Z,Gu J H.Laser OP- tronics Progr,1996; 7(Suppl):116 (方军,郑启光,王涛,陶星之,辜建辉,激光与光电子学进 展,1996;7(增刊):116) [9] Pei Y T Acta Metall Sin, 1998; 34: 987 (裴宇韬,金属学报,1998; 34: 987) [10] Flemings M C. Solidification Processing. New York :Mac- Graw-Hill,1974:194 [11] Xiong W H, Hu Z H, Cui K. Acta Metall Sin, 1996; 32:1075 (熊惟皓,胡镇华,崔,金属学报,1996;32:1075) [12]Zeng D L.Materials of Powder Metallurgy,Beijing:Metal- lurgical Industry Press,1989:174 (曾德麟,粉末冶金材料,北京:冶金工业出版社,1989:174) [13] Liu N, Hu Z H Cui K Acta Mate, Comp sin, 1996; 13(4): 39 刘宁,胡镇华,崔.复合材料学报,1996;13(4):39) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|