| TIAN Sugui ; ZHOU Huihua ; ZHANG Jinghua; YANG Hongcai ; XU Yongbo;HU Zhuangqi ( State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)( Department of Materials Science and Engineering; Northeastern University ; Shenyang 110006)( Department of Materials Science and Engineering; Shenyang Polytechnic University; Shenyang 110023)Correspondent: TIAN Sugui; associate professor Tel: (024)5927399 |
引用本文:
田素贵;周惠华;张静华;杨洪才;徐永波;胡壮麒. 一种单晶镍基合金蠕变期间γ'相的定向粗化机制[J]. 金属学报, 1998, 34(6): 591-596.
,
,
,
,
,
.
A DIRECTIONAL COARSENING MECHANISM OF THE γ'-PHASE DURING CREEP OF A SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. Acta Metall Sin, 1998, 34(6): 591-596.
1Tien J K, Copley S M. Metoall Trans, 1971; 2: 215 2 Nathalal M L, Ebert L J. Scr, Metall 1983; 17: 1151 3 Mackay R A,Ebert L J .Scr,Metall 1983;17:1217 4 Pollock T M, Argon A S. Acto Metall Mater 1994; 42: 1859 5 Glatzel U, Feller-Knirpmeier M. Scr Metall 1989; 23: 1839 6 Socrate S, Parks D M. Acto Metall Mater 1993; 41: 2185 7 Muller L, Glatzel U, Feller-Kniepmeier M. Acta Metall Mater 1992; 40: 1321 8 彭志方, Glatzel U, Feller—Kniepmeier M.金属学报, 1995; 31: A531 (Peng Z F ,Glatzel U,Feller—Kniepmeier M.Acta Metall Sin 1995;31:A531) 9 秦高梧,郝士明.金属学报,1995;31:B485 (Qin G W, Hao S M. Acta Metall Sin 。, 1995; 31: B485) 10Svetlov I L, Golovko B A, Epishin A I, Abalakin N P. Scr Metall Mater 1992; 26: 1353 11Duval S, Chambleland S, Caron P, Blavette D. Acto Metall Mater 1994; 42: 185 12 Pcollock T M,Argon A S.In:Kassanger R D,Deye D J eds.Superalloys ,Warrendale Pa:A I M E,1988:285 13 Veron M, Brechet Y, Louchet P. In: Kassanger R D, Depe D J eds. Superalloys, Warrendale, Pa: A I M E, 1996:181 14 Nabarro F R N. Metall Mater Trans , 1996; 27A: 513 |
|