| 1.25Cr-0.5Mo中温抗氢钢的回火析出相及其对抗氢蚀能力的影响 |
| 苏铁健;罗兴宏;范存淦;李依依;陈晓;郭爱民 |
| 中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;武汉钢铁公司;武汉;430080;武汉钢铁公司;武汉;430080 |
|
| TEMPERING PRECIPITATES OF STEEL 1.25Cr-0.5Mo AND THEIR EFFECTS ON ITS HYDROGEN ATTACK RESISTANCE |
| SU Tiejian; LUO Xinghong; FAN Cungan; LI Yiyi (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)CHEN Xiao; GUO Aimin (Wuhan Iron and Steel Company; Wuhan 430080)Correspondent: SU Tiejian; Fax: 024-3891320; Tel. 024-3843531-55445)(Manuscript received 1997-04-30; in revised form 1997-07-08) |
引用本文:
苏铁健;罗兴宏;范存淦;李依依;陈晓;郭爱民. 1.25Cr-0.5Mo中温抗氢钢的回火析出相及其对抗氢蚀能力的影响[J]. 金属学报, 1998, 34(4): 393-399.
,
,
,
,
,
.
TEMPERING PRECIPITATES OF STEEL 1.25Cr-0.5Mo AND THEIR EFFECTS ON ITS HYDROGEN ATTACK RESISTANCE[J]. Acta Metall Sin, 1998, 34(4): 393-399.
1 Shewmon P G,Mater Sci Technol. 1985;1:1-8 2 余宗森.钢的高温氢腐蚀. 北京:化学工业出版社,1987: 312(YU Zongsen. Hydrogen Attack at Elevated Temperature. Beijing: Chemistry Industrial Publication, 987:312) 3 Lundberg R, Waldenstrom M, Uhrenius B. CALPHAD; 1977; 1: 159 4 Odette G R, Vagarali S S Metall Trans, 1982; 13A: 299 5 Parthasarathy T A,Shewmon P G. Metall Trans, 1984; 15A:2021 6 Sundararajan G,Shewmon P G Metall Trans, 1980;11A:509 7 刘国勋.金属学原理北京:冶金工业出版社,1983:291(LIU Guoxun.Principle of Metal Science. Beijing:Metallurgical Industrial Publication, 1983:291) 8Senior B A. Mater Sci Eng, 1988; A103:263 |
|