| 定向凝固Ni_3Al合金高温变形后的显微组织特征 |
| 谷月峰;林栋梁;单爱党;陈家光;胡凡;曹涵清 |
| 上海交通大学国家教委高温材料及高温测试开放实验室;上海;200030;上海交通大学国家教委高温材料及高温测试开放实验室;上海;200030;上海交通大学国家教委高温材料及高温测试开放实验室;上海;200030;上海宝山钢铁研究所;上海;201900;上海宝山钢铁研究所;上海;201900;上海宝山钢铁研究所;上海;201900 |
|
| MICROSTRUCTURE FEATURES IN DIRECTIONALLY SOLIDIFIED Ni_3Al ALLOY AFTER HIGH TEMPERATURE DEFORMATION |
| GU Yuefeng; LIN Dongliang; SHAN Aidang (The Public Laboratory of State Education Commission for High Temperature Materials and High Temperature Tests; Shanghai Jiaotong University; Shanghai 200030)(CHEN Jiaguang; HU Fan; CAO Hanqing (Shanghai Baoshan Institute of Iron and Steel; Shanghai 201900) |
引用本文:
谷月峰;林栋梁;单爱党;陈家光;胡凡;曹涵清. 定向凝固Ni_3Al合金高温变形后的显微组织特征[J]. 金属学报, 1998, 34(4): 351-355.
,
,
,
,
,
.
MICROSTRUCTURE FEATURES IN DIRECTIONALLY SOLIDIFIED Ni_3Al ALLOY AFTER HIGH TEMPERATURE DEFORMATION[J]. Acta Metall Sin, 1998, 34(4): 351-355.
1 清木青,和泉修.日本金属学会志,1979;43:1190(Aoki K, Izumi O J Jpn Inst Met, 1979; 43: 1190) 2 Liu C T, White C L; Horton J A. Acta Metall, 1985; 33: 213 3谷月峰,林栋梁,单爱党,刘毅,刘震云.金属学报,1997; 33:325(Gu Yuefeng,Lin Dongliang (Lin T L),Shan Aidang, Liu Yi, Liu Zhenyun. Acta Metall Sin, 1997; 33:325) 4 谷月峰,林栋梁,单爱党、刘毅,叶伟.金属学报, 1996; 32: 1144 (Gu Yuefeng, Lin Dongliang(Lin T L), Shan Aidang, Liu Yi, Ye Wei. Acta Metall Sin, 1996; 32: 1144) 5谷月峰,刘 毅,林栋梁.郭建亭电子显微学报,1994;13:497(Gu Yuefeng,Liu Yi,Lin Dongliang(Lin T L),Guo Jianting.J Chin Electron Microscopy Soc, 19942 13:497) 6Gottstein G, Chang L, Yung H F. Mater Sci Technol, 1991; 7: 158 7Lin Dongliang(Lin T L); Shan A D, Li D Q Scr Metall Mater, 1994; 31: 1455 8Li D Q, Shan A D, Liu Y, Lin Dongliang(Lin T L). Scr Metall Mater, 1995; 33: 685 |
|