| Al_(65)Cu_(20)Cr_(15)准晶颗粒/铝基复合材料中二十面体准晶的扩散相变 |
| 齐育红;张占平;黑祖昆;全明秀;董闯 |
| 大连海事大学金属材料工艺研究所;大连;116026;大连海事大学金属材料工艺研究所;大连;116026;大连海事大学金属材料工艺研究所;大连;116026;中国科学院金属研究所;沈阳;110015;大连理工大学;大连;116024 |
|
| DIFFUSION-CONTROLLED PHASE TRANSFORMATIONS OF Al_(65)Cu_(20)Cr_(15) QUASICRYSTALLINE PARTICLES/AI MATRIX COMPOSITES |
| QI Yuhong;ZHANG Zhanping;HEI Zukun (Institute of Metal and Technology; Dalian Maritime University; Dalian 116026)QUAN Mingliu (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)DONG Chuang (Dalian University of Technology; 116024) |
引用本文:
齐育红;张占平;黑祖昆;全明秀;董闯. Al_(65)Cu_(20)Cr_(15)准晶颗粒/铝基复合材料中二十面体准晶的扩散相变[J]. 金属学报, 1998, 34(1): 19-23.
,
,
,
,
.
DIFFUSION-CONTROLLED PHASE TRANSFORMATIONS OF Al_(65)Cu_(20)Cr_(15) QUASICRYSTALLINE PARTICLES/AI MATRIX COMPOSITES[J]. Acta Metall Sin, 1998, 34(1): 19-23.
1 Shechtman D, Blech I,Cahn J W.Phys Rev Lett;1984;53:1951 2 Kang S S,Dubois J M J Mater Res,1993; 8:2471 3 Tsai A P, Aoki K;Inove A.Masumoto T J Mater Res.1993;8:5 4 齐育红.张占平.黑祖昆,严立.摩擦学学报,1997;待发表(Qi Yuhong,Zhang Zhanping;Hei Zukun,Yan Li.Tribology;1997,to be published) 5 Bondersky L.Phys Rev Lett,1985; 54: 2422 6 Selke H; Ryder P L Mater Sci Eng, 1993; A165: 81 |
|