| 45钢淬火过程中热传导方程逆问题求解 |
| 程赫明;王洪纲;陈铁力 |
| 昆明理工大学;昆明;650093;昆明理工大学;昆明;650093;昆明理工大学;昆明;650093 |
|
| SOLUTION OF HEAT CONDUCTION INVERSE PROBLEM FOR STEEL 45 DURING QUENCHING |
| CHENG Heming;WANG Honggang;CHEN Tieli (Kunming University of Science and Technology; Kunming 650093) |
引用本文:
程赫明;王洪纲;陈铁力. 45钢淬火过程中热传导方程逆问题求解[J]. 金属学报, 1997, 33(5): 467-472.
,
,
.
SOLUTION OF HEAT CONDUCTION INVERSE PROBLEM FOR STEEL 45 DURING QUENCHING[J]. Acta Metall Sin, 1997, 33(5): 467-472.
1Prince R F,Fletcher A J.Met Technol,1980;2:203 2Denis S,Farias D,Simon A.ISIJ Int,1992;32:316 3Tzitzlkov I,Hougardy H P,Rose A.Arch Eisenhuttenwes,1974;45:525 4Majorek A.Programmdokumentation.Institut fuer Werkstoffkunde,University Karlsruhe,1992:42 5Adams J A,Rogers D F.Computer-aided Heat Transfer Analysis.New York:McGraw-Hill.1973:145 6Bates C E,Totten G E,Brennan R L.ASM Int,1991;2:72 |
|