| 定向凝固钢锭中宏观偏析的预测 Ⅰ.数学模型 |
| 顾江平;刘庄;陈晓慈 |
| 清华大学;北京;100084;清华大学;北京;100084;中国第二重型机械集团公司;德阳;618013 |
|
| PREDICTION OF MACROSEGREGATION OF UNIDIRECTIONALLY SOLIDIFIED STEEL INGOTS Ⅰ. MATHEMATICAL MODEL |
| GU Jiangping;LIU Zhuang (Tsinghua University; Beijing 100084); CHEN Xiaoci(The Second Heavy Machinery Group Company of China; Deyang 618013) |
引用本文:
顾江平;刘庄;陈晓慈. 定向凝固钢锭中宏观偏析的预测 Ⅰ.数学模型[J]. 金属学报, 1997, 33(5): 461-466.
,
,
.
PREDICTION OF MACROSEGREGATION OF UNIDIRECTIONALLY SOLIDIFIED STEEL INGOTS Ⅰ. MATHEMATICAL MODEL[J]. Acta Metall Sin, 1997, 33(5): 461-466.
1 Bennon W D,Incropera F P.Int J Heat Mass Transfer,1987;30:21 2 Voller V R,Prakash C.Int J Heat Mass Transfer,1987;30:1709 3 Beckerman C,Viskanta R. Phys Chem Hydrodyn,1988:12:1995 4徐达鸣,李庆春.金属学报,1990;26:B267 5樱井隆,山田人久.铁钢.1986;72:5188 6大中逸雄,松本雅庆.铁钢,1987;73:1698 7 Batte T P Int Maler Re八 1992 37: 249 SKagawaA,OkamotoT.MatersciTechnol,1986;2:9977Battle T P.Int Mater Rev,1992;37:249 8Kagawa A,Okamoto T.Mater Sci Technol,1986;2:997 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|