| 42CrMo钢在非比例循环加载下的塑性流动分析 |
| 杨显杰;高庆;蔡力勋;陈旭;袁珩 |
| 西南交通大学 |
|
| PROPERTIES OF PLASTIC FLOW OF STEEL 42CrMo UNDER NONPROPORTIONAL CYCLIC LOADING |
| YANG Xianjie; GAO Qing; CAI Lixun; CHEN Xu; YUAN Heng(Southwest Jiaotong University;Chengdu; 610031) |
引用本文:
杨显杰;高庆;蔡力勋;陈旭;袁珩. 42CrMo钢在非比例循环加载下的塑性流动分析[J]. 金属学报, 1995, 31(4): 170-176.
,
,
,
,
.
PROPERTIES OF PLASTIC FLOW OF STEEL 42CrMo UNDER NONPROPORTIONAL CYCLIC LOADING[J]. Acta Metall Sin, 1995, 31(4): 170-176.
| 1杨显杰,高庆,孙训方.航空学报,1994;15:12612 TanakaE,MurakamiS,OokaM.JMechPhysSolids,1985;33:5593 NingJ,ChenX.IntJSolidsStruct,1991;28(4):4034彭向和,高芝晖,马鸣图,颜在先.金属学报,1993;29:A429x |
|