金属学报  1995, Vol. 31 Issue (16): 164-172    
  论文 本期目录 | 过刊浏览 |
离子束增强沉积氮化硅膜及TiAl抗高温氧化性能的改善
徐东;朱宏;汤丽娟;杨云洁;郑志宏;柳襄怀;谷口滋次;柴田俊夫
中国科学院上海冶金研究所离子束开放实验室;日本大阪大学材料系
IMPROVEMENT OF OXIDATION RESISTANCE OF TiAl BY ION-BEAM-ENHANCED DEPOSITION OF Si_3N_4 COATINGS
XU Dong;ZHU Hong; TANG Lijuan;YANG Yunjie; ZHENG Zhihong; LIU Xianghuai(Ion Beam Laboraiory; Shanghai Institute of Metallurgy; Chinese Academy of Sciences; Shanghai 200050) TA NIGUCHI S; SHIBATA T(Department of Materi als Science and Processing; Faculty of Engineering; Osaka University; Japan)(Manuscript received 1994-02-19; in revised form 1994-11-30)
引用本文:

徐东;朱宏;汤丽娟;杨云洁;郑志宏;柳襄怀;谷口滋次;柴田俊夫. 离子束增强沉积氮化硅膜及TiAl抗高温氧化性能的改善[J]. 金属学报, 1995, 31(16): 164-172.
, , , , , , , . IMPROVEMENT OF OXIDATION RESISTANCE OF TiAl BY ION-BEAM-ENHANCED DEPOSITION OF Si_3N_4 COATINGS[J]. Acta Metall Sin, 1995, 31(16): 164-172.

全文: PDF(733 KB)  
摘要: 用离子束增强沉积(IBED)方法在金属间化合物TiAl上合成厚度为0.5,1,和2μm的氮化硅薄膜。所形成的薄膜为非晶态,膜与基底间存在混合的过渡区,膜与基底结合紧密用AES,XRD和XPS研究薄膜的组成和结构,高温循环氧化结果表明,经沉积膜的TiAl试样的抗氧化性能显著提高其中沉积0.5μm薄膜的试样表现出极好的抗循环氧化性能由SEM及EDS分析得出,良好的高温稳定性能、高的膜/基底结合力和形成富Al2O3和硅化物的保护层是提高TiAl抗高温氧化性能的主要因素.
关键词 : 氮化硅薄膜,  TiAl,  离子束增强沉积,  高温氧化    
Abstract:Silicon nitride films were synthesized by ion-beam-enhanced-deposition (IBED) on an IBED system. Auger electron spectroscopy, X-ray diffraction (XRD). X-ray photoemission spectroscopy (XPS) and the scratch test were performed for investigating the composition. structure and the adhesion with the substrate of them. It was found that the silicon nitride film is composed of a thin silicon enriched top layer. a stoichiometric Si3N4 layer and a mixing layer at the film-substrate interface. Cyclic oxidation tests were carried out on the TiAl coated with the silicon nitride films of thicknesses of 0.5. 1 and 2 μm. The results revealed that IBED silicon nitride film is effective to improve the oxidation resistance of TiAl at high temperature. The 0.5 μm silicon nitride film demonstrated an excellent oxidation resistance at 1300 K for at least 30 cycle (600 h). However, this effect decreases as the thickness of coating increases. SEM and energy-dispersive X-ray spectroscopy revealed that the excellent oxidation resistance came from the formation of a thin layer rich in Al2O3 and silicon compound beneath the outer TiO2thin layer. (Correspondent: LIU Hianghuai, Professor, Shanghai Institute of Metallurgy, Chinese Academy of Sciences,Shanghai,200050)
Key words: Si3N4 film. TiAl. ion beam enhanced deposition. oxidation resistance
    
1TaniguchiS,ShibataT,TakeuchiK.MalerTransJpmInstMet.1991;32:2992PerkinsRA,ChingKT,MeverGH.ScrMet,1987:21:15053KasaharaK,HashimotoK,DoiH,TsujimotoT.JJpnInstMet,1989;53:584UmakoshiY,YamaguchiM,SakagamiT,YamaneT.JMalerSci,1989;24:15995TaniguchiS,ShibataT,ItohS.MaterTransJpnInstMet,1991:32:1516TaniguchiS,LiuXianghuaiet.al.,MalerSciEng,1989;A121:5197LiuXianghuai,XueBin,ZhengZhihong,ZhouZuyao,ZouShichang.NuclInstrMethPhysRes.1989:B39:1858ZhouJiankun,Biersack JP,FinkD,MaterLett.1991;10(11):532
[1] 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江. 镁合金抗高温氧化机理研究进展[J]. 金属学报, 2023, 59(3): 371-386.
[2] 王虎, 赵琳, 彭云, 蔡啸涛, 田志凌. 激光熔化沉积TiB2 增强TiAl基合金涂层的组织及力学性能[J]. 金属学报, 2023, 59(2): 226-236.
[3] 徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生. 微量Al、Ti对Inconel 690合金高温氧化行为的影响[J]. 金属学报, 2023, 59(12): 1547-1558.
[4] 李小兵, 潜坤, 舒磊, 张孟殊, 张金虎, 陈波, 刘奎. W含量对Ti-42Al-5Mn-xW合金相转变行为的影响[J]. 金属学报, 2023, 59(10): 1401-1410.
[5] 沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐. SiCf/TiAl复合材料界面反应及热稳定性[J]. 金属学报, 2022, 58(9): 1150-1158.
[6] 刘仁慈, 王鹏, 曹如心, 倪明杰, 刘冬, 崔玉友, 杨锐. 700℃热暴露对 β 凝固 γ-TiAl合金表面组织及形貌的影响[J]. 金属学报, 2022, 58(8): 1003-1012.
[7] 解磊鹏, 孙文瑶, 陈明辉, 王金龙, 王福会. 制备工艺对FGH4097高温合金微观组织与性能的影响[J]. 金属学报, 2022, 58(8): 992-1002.
[8] 丛鸿达, 王金龙, 王成, 宁珅, 高若恒, 杜瑶, 陈明辉, 朱圣龙, 王福会. 新型无机硅酸盐复合涂层制备及其在高温水蒸气环境的氧化行为[J]. 金属学报, 2022, 58(8): 1083-1092.
[9] 陈玉勇, 叶园, 孙剑飞. TiAl合金板材轧制研究现状[J]. 金属学报, 2022, 58(8): 965-978.
[10] 杨亮, 吕皓天, 万春磊, 巩前明, 陈浩, 张弛, 杨志刚. 综述:活性元素作用机理——氧化物“钉扎”模型[J]. 金属学报, 2021, 57(2): 182-190.
[11] 李天瑞, 刘国怀, 于少霞, 王文娟, 张风奕, 彭全义, 王昭东. 直接包套轧制铸态Ti-46Al-8Nb合金的组织特征及热变形机制[J]. 金属学报, 2020, 56(8): 1091-1102.
[12] 刘先锋, 刘冬, 刘仁慈, 崔玉友, 杨锐. Ti-43.5Al-4Nb-1Mo-0.1B合金的包套热挤压组织与拉伸性能[J]. 金属学报, 2020, 56(7): 979-987.
[13] 王希,刘仁慈,曹如心,贾清,崔玉友,杨锐. 冷却速率对β凝固γ-TiAl合金硼化物和室温拉伸性能的影响[J]. 金属学报, 2020, 56(2): 203-211.
[14] 赵明雨,甄会娟,董志宏,杨秀英,彭晓. 新型耐磨耐高温氧化NiCrAlSiC复合涂层的制备及性能研究[J]. 金属学报, 2019, 55(7): 902-910.
[15] 陈占兴,丁宏升,陈瑞润,郭景杰,傅恒志. 脉冲电流作用下TiAl合金凝固组织演变及形成机理[J]. 金属学报, 2019, 55(5): 611-618.