| Fe—1.83C马氏体中碳的有序化 Ⅱ.长周期有序相的晶体结构 |
| 任晓兵;王笑天 |
| 西安交通大学;南京大学物理系 |
|
| CARBON ORDERING IN Fe-C MARTENSITE Ⅱ. Crystal Structure of Long-Period Ordered Phase |
| REN Xiaobing; Xiaotian(Xi'an Jiaotong University); SHIMIZU Ken'ichi(Kanazawa Institute of Technology;Japan) TADAKI Tsugio(Osaka University; Japan) |
引用本文:
任晓兵;王笑天. Fe—1.83C马氏体中碳的有序化 Ⅱ.长周期有序相的晶体结构[J]. 金属学报, 1994, 30(8): 337-343.
,
.
CARBON ORDERING IN Fe-C MARTENSITE Ⅱ. Crystal Structure of Long-Period Ordered Phase[J]. Acta Metall Sin, 1994, 30(8): 337-343.
| 1NagakuraS,ToyoshimaM.TransJpnInstMet,1974;15:1292NagakuraS,HirotsuY,KusunokiM,NakaimuraYMetallTrans,1983;14A:10253TanakaY,ShimizuKTransJpnInstMet,1981;22:7794TaylorKA,ChangL,OlsonGB,SmithGDW,CohenM,VanderSandeJB.MetallTrans,1989;20A:27175UwakwehONC,GeninJMR,SilvainJGMetallTrans22A:7976OlsonCB,TaylorKA,CohenM.MetallTrans1990;21A:28067任晓兵,王笑天,清水谦一,唯木次男.金属学报,1994:30:A2968任晓兵,王笑天,清水谦一,唯木次男,金属学报,1994,30.A2899JohannsonCH,LindeJOAnnPhys,1936;25:110FujiwaraKJPhysSocJpn.1957,12:711OgawaSIn:WarlimountHedProcIntSymponOrder-DisorderTransformationsinAlloys,1974:24012YakelHLJApplPhys1962,13:243913GanguleeA,MossSC.JApplCrystallogr,1968;1:61 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|