| TiAl基合金组织对拉伸性能的影响 |
| 蒲忠杰;石建东;邹敦叙;仲增墉 |
| 高级工程师;北京(100081);冶金工业部钢铁研究总院五室;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| EFFECT OF MICROSTRUCTURE ON TENSILE PROPERTIES OF TiAl BASED ALLOYS |
| PU Zhongjie;SHI Jiandong;ZOU Dunxu;ZHONG Zengyong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijingsenior engineer;Department No.5; Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081 |
引用本文:
蒲忠杰;石建东;邹敦叙;仲增墉. TiAl基合金组织对拉伸性能的影响[J]. 金属学报, 1993, 29(8): 31-36.
,
,
,
.
EFFECT OF MICROSTRUCTURE ON TENSILE PROPERTIES OF TiAl BASED ALLOYS[J]. Acta Metall Sin, 1993, 29(8): 31-36.