Cr-Zn-Al合金溶质原子贫化区贝氏体切变形核的原位观察 |
孟祥康;康沫狂 |
博士生;西安(710072);西北工业大学401教研室;西北工业大学 |
|
IN SITU OBSERVATION OF BAINITIC NUCLEATION BY SHEAR IN SOLUTE DEPLETED ZONE IN Cu-Zn-Al ALLOY |
MENG Xiangkang;KANG Mokuang Northwestern Polytechnical Uiversitydoctoral candidate;Faculty 401;Norhtwestern Polytchnical University; Xi'an 710072 |
引用本文:
孟祥康;康沫狂. Cr-Zn-Al合金溶质原子贫化区贝氏体切变形核的原位观察[J]. 金属学报, 1993, 29(8): 25-30.
,
.
IN SITU OBSERVATION OF BAINITIC NUCLEATION BY SHEAR IN SOLUTE DEPLETED ZONE IN Cu-Zn-Al ALLOY[J]. Acta Metall Sin, 1993, 29(8): 25-30.
1 Kurdjumov G. Trans AIME. 1933; 105:253 2 Entin R I. In: Zackay V E, Aaronson H I eds., Decomposition of Austenite by Diffusional Processes, New York: John Willey, 1962: 295 3 Lim C, Wutting M. Acta Metall. 1974; 22: 1215 4 谢朝阳,康沫狂,材料科学进展,1990;4:161 5 杨全民,康沫狂,金属学报,1990;26:A235 6 Takezawa K, Sato S. Proc Inter Conf on Martensitic Transformation, Nara, The Japan Institute of Metals, 1986: 625 7 Takezawa K, Sato S. Metall. Trans., 1990; 21A: 1541 8 徐祖耀,上海金属,1991;13:7 9 徐祖耀,上海金属,1992;14:8 10 Meng X K, Kang M K, Yang Y Q, Liu D H. Metall. Trans., 1993; 24A: in press 11 杨全民,西北工业大学博士学位论文,西安,1989:32 12 Kang M K, Yang Y Q, Wei Q M, Meng X K. Metall. Trans., 1993; 24A: in press 13 张骥华,陈树川,徐祖耀,金属学报,1986;22:A372 14 张骥华,陈树川,徐祖耀,材料科学进展,1989;3:105 15 Zhao Z Q, Chen F X, Yang D Z. J Phys: Condens Matter, 1989; 1: 1395 16 赵增祺,陈绯瑕,杨大智,包耳,第二届全国贝氏体相变讨论会论文集,峨眉,1990;101 17 沈惠敏,芮煜明,张志方,袁方,王业宁,第三届全国马氏体相变会议论文集,秦皇岛;1990:137 18 张丽萍,李福全,张恩涛,邓肇豪,机械工程材料,1990;14:7 19 魏秋明,西北工业大学博士学位论文,西安,1991:30 20 Chattopadhyay K, Aaronson H I.Acta Metall., 1984; 34: 695 21 Guenin G, Cobin P F. Metall. Trans. 1982; 13A: 1127 22 Cliff G, Hasan F, Lorimer G W, Kikuchi M. Metall. Trans., 1990; 21A: 831 23 Wu M H, Wayman C M. Proc Inter Conf on Martensitic Transformation, Nara, The Japan Institute of Metals, 1986: 619q |
|