| 计算晶粒尺寸分布的几何模型及实用方法 |
| 赵新兵;K.LüCKE |
| 浙江大学;德国亚琛工业大学 |
|
| GEOMETRIC MODEL AND APPLIED METHOD FOR CALCULATION OF GRAIN SIZE DISTRIBUTIONS |
| ZHAO Xinbing(Zhejiang University; Hangzhou) KLüCKE (Institut fur Metallkunde und Metallphysik der R WTH Aachen; Germany) |
引用本文:
赵新兵;K.LüCKE. 计算晶粒尺寸分布的几何模型及实用方法[J]. 金属学报, 1992, 28(8): 17-24.
,
.
GEOMETRIC MODEL AND APPLIED METHOD FOR CALCULATION OF GRAIN SIZE DISTRIBUTIONS[J]. Acta Metall Sin, 1992, 28(8): 17-24.
1 Rhines F N, Craig K R, Rousse D A. Metall Trans, 1976; 7A: 1729-1734 2 Rhines F N, Patterson B R. Metall Trans, 1982; 13A: 985-993 3 Exner H E. Int Metall Rev, 1972; 17: 25-42 4 Wicksell S D. Biometrika, 1925; 17: 84-99 5 Scheil E. Z Anorg Chem, 1931; 201: 259-264 6 Scheil E. Z Metallk, 1935; 27: 199-209 7 Exner H E. Z Metallk, 1966; 57: 755-763 8 Saltykov S A. Stereometric Metallography. 2nd ed., Moscow: Metallurgizdat, 1958 9 Bockstiegel G. Z Metallk, 1966; 57: 647-652 10 DeHoff R T, Liu Guoquan. Metall Trans, 1985; 16A: 2007-2011q |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|