| γ-Fe中硼的扩散机制 |
| 余宗森;陈宁 |
| 北京科技大学;北京科技大学 |
|
| MECHANISM FOR DIFFUSION OF BORON IN γ-Fe |
| YU Zongsen;CHEN Ning University of Science and Technology Beijing |
引用本文:
余宗森;陈宁. γ-Fe中硼的扩散机制[J]. 金属学报, 1992, 28(3): 10-14.
,
.
MECHANISM FOR DIFFUSION OF BORON IN γ-Fe[J]. Acta Metall Sin, 1992, 28(3): 10-14.
1 Busby P E, Warga M E, Wells C. Trans AIME, 1953; 197: 1463 2 Schuman H. Metallurgie Giessereitechnik, 1954; 4: 305 3 Grange R A, In: Grange R A, Shortsleeve F J, Hilty D C, Binder W O, et al. eds., Boron, Calcium, Columbium and Zirconium in Iron and Steel. New York: John Wiley & Sons, 1957: 11 4 Goldhoff R M. J Met, 1957; 10: 1278 5 Williams T M, Stoneham A M, Harries D R. Met Sci, 1976; 10: 14 6 Chapman M A V, Faulkner R G. Acta Metall 1983; 31: 677 7 Shewmon P G. Diffusion in Solide. New York: McGraw-Hill, 1990: 115 8 贺信莱,褚幼义,张秀林,余宗森,李秋萍,尹熙光.金属学报,1977;13:235 9 Karlsson L, Norden H, Odelius H. Acta Metall, 1988; 36: 1--12. Karlsson L. Acta Metall, 1988; 36: 13--34. Karlsson L, Norden H. Acta Metall, 1988; 36: 35--48 10 Hashimoto M, Ishida Y, Yamamoto R, Doyama M. Acta Metall, 1984; 32: 1 11 Johnson R A. J Phys F: Metal Physics, 1973; 3: 295 12 Seibel G, Acod C R. Acad Sci Paris, 1963; 256: 4661 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|