| 马氏体相变研究的进展和瞻望 |
| 徐祖耀 |
| 上海交通大学 |
|
| SOME ASPECTS OF PROGRESS AND PERSPECTIVE IN MARTENSITIC TRANSFORMATION |
| XU Zuyao T. Y. Hsu Shanghai Jiaotong University |
引用本文:
徐祖耀. 马氏体相变研究的进展和瞻望[J]. 金属学报, 1991, 27(3): 1-12.
.
SOME ASPECTS OF PROGRESS AND PERSPECTIVE IN MARTENSITIC TRANSFORMATION[J]. Acta Metall Sin, 1991, 27(3): 1-12.
1 Osmond F. Bull Soc Encour Ind Nat, 1895; 10: 480 2 Bain E C. Trans AIME, 1924; 70: 25 3 Greninger A B, Mcoradian V G, Trans AIME, 1938; 128: 337 4 Greninger A B. Trans AIME, 1939; 129: 1 5 徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980 6 徐祖耀.相变原理.北京:科学出版社,1988 7 Nishiyama Z. Fine M E, Meshii M, Wayman C M. Martensitic Transformation, New York: Academic Press, 1978 8 Cohen M. Phase Transformations in Solids, New York: John Wiley & Sons, 1951: 588 9 Barrett C S. Transformations in Solids, New York: John Wiley & Sons, 1951: 343 10 Troiano A R, Greninger A B. Met prog, 1946; 50: 303 11 1948; 18: 999 12 1948; 61: 83 13 1949; 66: 761 14 Greninger A B, Troiano A R. Trans AIME, 1949; 185: 590 15 Bowles J S. Acta Crystallogr, 1951; 4: 162 16 Wechsler M S, Lieberman D S, Read T A. Trans AIME, 1953; 197: 1503 17 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129, 138, 224 18 Hull D. Bull Inst Met, 1954; 2: 134 19 Bilby B A, Christian J W. The Mechanism of Phase Transformations in Metals, Inst Metals Monograph No.18, London, 1956: 121 20 Christian J W. Physical Properties of Martensite and Bainite, Spl. Rep. 93, Iron and Steel Inst, London, 1965:1 21 Clark H M, Wayman C M Phase Transformations, Metals Park, Ohio: ASM, 1970: 59 22 Cohen M, Olson G B, Clapp P C. Proc ICOMAT-79, MIT, Cambridge. Mass, 1979: 1 23 Wayman C M. Martensitic Transformations, Proc ICOMAT-89, Materials Science Forum, 56-58, 1990: 1 24 Olson G B. Martensitic Transformations, Proc ICOMAT-89, Materials Science Forum. 56-58. 1990: 89 25 Rao B V N, Thomas G. Proc Int Conf on Martensitic Transformations, ICOMAT-1979, MIT, Cambridge, Mass., 1979: 12 26 Thomas G, Sarikaya M. Proc Int Conf on Solid-solid Phase Transformations, TMS-AIME, 1982: 999 27 徐祖耀,李学敏.金属学报,1983;19:A83 28 徐祖耀,李学敏.金属学报,1983;19:A505 29 Hsu T Y, Li Xuemin. Ser Metall, 1983; 17: 1285 30 Hsu T Y, Chen Yixin, Chen Weiye. Matall Trans, 1987; 18A: 1389 31 徐祖耀,陈业新,陈伟业.钢铁,1990;25(1) :38
32 Hsu T Y (徐祖耀). Proc ICOMAT-86, Key note lecture, The Japan Inst Metals, 1987: 245 33 徐祖耀.材料科学进展,1987;1(4) :3 34 徐祖耀.材料科学与工程,1989;7(2) :18 3S 徐祖耀.金属学报,1979;15:329 36 徐祖耀.金属学报,1980;16:420 37 徐祖耀.金属学报,1980;16:426 38 Hsu T Y(徐祖耀), J Mater Sci, 1985: 20: 23 39 Hsu T Y(徐祖耀), Zhang Hongbing, Luo Shoufu. J Mater Sci, 1983; 18: 3026 40 Hsu T Y(徐祖耀), Zhang Hongbing, Acta Metall, 1984; 32: 343 41 徐祖耀,张鸿冰,罗守福.金属学报,1984;20:A151 42 Zhang Hongbing. Hsu T Y (徐祖耀). Acta Metall, 1986: 34: 333 43 张鸿冰,倪乐民,徐祖耀.金属学报,1987;23:A42 44 潘牧,徐祖耀.材料科学进展,1988;2(5) :32 45 徐祖耀,潘牧.金属学报,1989;25:A250 46 李箭,徐祖耀.金属学报,1987;23:A321 47 李麟,徐祖耀.金属学报,1984;20:A112 48 李麟,徐祖耀.金属热处理学报,1985;6(2) :44 49 Li Lin, Hsu T Y (徐祖耀). Proc 4th Int Congress on Heat Treatment of Materials, IFHT, Vol.1. 1985: 343 50 Li Lin, Hsu T Y (徐祖耀). J Heat Treat, 1985; 4: 140 51 徐祖耀.材料科学进展,1988;2(6) :1 52 Hsu T Y (徐祖耀), Shape Memory Alloy '86, China Academic, pub. 1986; 207 53 Wu Jianxin, Jiang Bohong, Hsu T Y(徐祖耀). Acta Metall, 1988; 36: 1521 54 Hsu T Y (徐祖耀). Martensitic Transformations, Proc ICOMAT-89, Materials Science Forum 56--58, 1990: 145 55 Ortin J, Planes A. Acta Metall, 1988; 36: 1873 56 Ortin J, Planes A. Martensitic Transformations, Proc ICOMAT-89, Materials Seience Forum, 56--58, 1990: 139 57 Hsu T Y (徐祖耀), Zhou Xiaowang. Acta Metall, 1989; 37: 3091 58 徐祖耀,周晓望.材料科学进展,1989;3:385 59 周晓望,徐祖耀.材料科学进展,1991;5(3) : 60 周晓望,徐祖耀.待发表 61 Hsu T Y (徐祖耀), Yan Linfah. J Mater Sci, 1983; 18: 3213 62 Hsu T Y (徐祖耀), Yan Linfah. Metallography. 1984; 17: 397 63 徐祖耀,颜林发.金属学报,1984;20:A143 64 颜林发,徐祖耀.金属学报,1986;22:A385 65 Tong H C, Wayman C M, Acta Mctall, 1975; 23: 209 66 吴建新,江伯鸿,徐祖耀.金属学报,1989;25:A98 67 Breinan E M, Ansell G S. Metall Trans, 1970; 1: 1513 68 徐祖耀,李箭,曾振鹏.金属学报,1986;22:A494 69 Hsu T Y (徐祖耀), Li Jian, Zen Zhengbang. Metallography. 1986; 19: 305 70 Hsu T Y (徐祖耀), Chen Weizhong, Scr Metall, 1987; 21: 1289 71 徐祖耀,陈卫中.金属学报,1988;24:A15 72 潘牧,徐祖耀.金属学报,1989;25:A389 73 Hassen P. In: Nabarro F R N ed, Dislocation in Solids, Vol.4, Amsterdan: North-Holland, 1979: 155 74 Magee C L. Phase Transformations, Metals Park, Ohio: ASM, 1970: 115 75 Gupta S K, Raghavan V. Acta Metall, 1975: 23: 1239 76 Kessler H, Pitsh W. Acta Metall. 1965; 13: 871 77 Kaufman L, Cohen M. The Mechanism of Phase Transformations in Metals, Inst Metals Monograph No.18. London, 1956: 187 78 Cohen M, Wayman C M. Metallurgical Treatises, TMS-AIME, 1981: 445 79 Cech R E, Turnball D. Trans AIME, 1956; 206: 124 80 Kachi Y, Bando Y, Higuchi S. Jpn J Appl Phys, 1962; 1: 307 81 Kaufman L, Cohen M. Prog Metal Phys, Vol.7, Pergamon Press, 1958: 165 82 Kaufman L. Leyenaar A, Harvey J S. Acta Metall, 1960; 8: 270 83 Korenko M K, Cohen M. Scr Metall, 1974; 8: 751
84 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897, 1905, 1915 85 Kajiwara S. Proc ICOMAT 79, MIT, Cambridge, Mass, 1979: 302 86 Kajiwara S. Metall Trans, 1986; 17A: 1701 87 Saburi T, Nenno S. Proc ICOMAT-86, Japan Inst Metals, 1987: 671 88 Kajiwara S. Philos Mag, 1981; A43: 1483 89 张星泉,贺贤铭.金属学报,1985;21:A175 91 刘禹门,李汾兰.金属热处理学报,1989;10(1) :1 91 Heuer A H, Ruhle M. Acta Metall, 1985; 33: 2101 92 Christian J W. Proc R Soc, 1951; A206: 51 93 Machlin E S, Cohen M. Trans AIME, 1952; 194: 489 94 Cahn J W. Acta Metall, 1957; 5: 168 95 Clapp P C. Phys Status Solidi, 1973; B57: 561 96 Clapp P C. Ferroelectrics, 1977; 16: 89 97 Suezawa M. Cook H. E. Acta Metall, 1980; 28: 423 98 Guenin G, Gobin P F. Metall Trans, 1982; 13A; 1127 99 Roitburd A L. Kristallografiya. 1962; 7: 291 Roitburd A L. Solid State Phys, 1978; 33: 317 100 Suzuki T, Wuttig M. Acta Mctall, 1975; 23: 1069 101 Olson G B, Cohen M. J Phys, (Paris), 1982; 43 (C4) : 75 102 Olson G B, Cohen M. Proc ICOMAT-86, Japan Inst Metals, 1987: 25--34 103 Guenin G, Clapp P C. Proc ICOMAT-86, Japan Inst Metals, 1987: 171--179 104 Clapp P C. Phase Transformations'87, Inst of Metals, London, 1988: 391 105 Clapp P C. Presented at CALPHAD XVII, Berkley, CA, July, 1988 106 Brooks J W, Loretto M H, Smallman R E. Acta Mctall, 1979; 27: 1829, 1839 107 Clapp P C. 私人通讯, 1989. 108 Cahn J W. Acta Metall, 1956; 4 449 109 Li Xuemin, Hsu T Y (徐祖耀). Mater Sci Eng, 1987; 91: 189 110 Li Xuemin, Hsu T Y (徐祖耀). In: Hasiguti R R et al. eds., Proc Second Sino-Japanese Mctal Physics and Physical Metallurgy Seminar, Sept. 25--27, 1986, Kunming, China, Japan-China Science and Tech. Association, Tokyo, Japan, 1988: 1 111 徐祖耀.上海金属,有色分册,1989;IO(2) :1 112 徐祖耀.稀有金属,1989;13:502 113 Tanner L E. Philos Mag, 1986; 14: 111 114 Kainuma T. Watanable R. J Jpn Inst Met, 1971; 35: 1126 115 Philips V A, Tanner L E. Acta Metall, 1973; 21: 441 116 Tanner L E. Pelton A R, Gronsky R. J Phys (Paris), 1982; 43(C4) : 169 117 Barsch G R, Krumhansi J A, Tanner L E, Wuttig M. Scr Metall, 1987; 21: 1257 118 Robertson I M. Wayman C M. Philos Mag, 1983; A 48: 421, 443, 629 119 Clapp P C. Rifkin J, Kenyon J, Tanner L F. Metall Trans, 1988; 19A: 783 120 Shapiro S M. Martensitic Transformations. Proc ICOMAT 89, Materials Science Forum, 56--58, 1990: 33 121 Yu Zhenzhong, Clapp P C. Metall Trans, 1989; 20A: 1601, 1617 122 朱伟光,徐祖耀.1984年第一届全国马氏体相变讨论会文集,Vol.1,1984:215 123 Jaswon M A, Wheeler J A. Acta Crystallogr, 1948; 1: 216 124 Tadaki T, Shimizu K. Trans Jpn Inst Met, 1970; 11: 44 125 Bowles J S, Dunne D P. Acta Metall, 1969; 17: 677 126 Acton A F. Beris M. Mater Sci Eng, |
|
Viewed |
|
|
|