| 非平衡Fe-Pd合金的热稳定性与磁性 |
| 张胜良;翟宏如 |
| 南京大学物理系;讲师南京(210008);南京大学 |
|
| THERMAL STABILITY AND MAGNETIC PROPERTIES OF NON-EQUILIBRIUM Fe-Pd ALLOYS |
| ZHANG Shengliang;ZHAI Hongru Nanjing University |
引用本文:
张胜良;翟宏如. 非平衡Fe-Pd合金的热稳定性与磁性[J]. 金属学报, 1991, 27(2): 48-51.
,
.
THERMAL STABILITY AND MAGNETIC PROPERTIES OF NON-EQUILIBRIUM Fe-Pd ALLOYS[J]. Acta Metall Sin, 1991, 27(2): 48-51.
1 Mader S. J Vac Sci Technol. 1965; 2: 35 2 Hassen M, Anderko K. Coustitution of Binary Alloys, New York: McGraw-Hill, 1958: 677 3 隅山兼治,日本金属学会会报,1986;25:615 4 Zhang S L, Sumiyama K, Nakamura Y. J Magn Magn Mater, 1988; 73: 58 5 Moruzzi V L, Marcus P M, Schwarz K. Mohn P. Phys Rev, 1986; B34: 1784 6 Hamada N. J Phys Soc Jpn, 1979; 46: 1759 7 Muraoka Y, Shiga M, Yasuoka H, Nakamura Y. J Phys Soc Jpn. 1976; 40: 414 8 Pearson W B. A Handbook of Lattice Spacings and Structures of Metals and Alloys. New York: Pergamon, 1958: 633 9 Kouvel J S, Wilson R H. J Appl Phys, 1961; 32: 435 |
|