| 电磁搅拌对低硫钢枝晶组织及机械性能的影响 |
| 胡汉起;郑日琪 |
| 教授;北京(100083);北京科技大学铸工教研室;北京科技大学 |
|
| INFLUENCE OF ELECTROMAGNETIC STIRRING ON DENDRITIC STRUCTURE AND MECHANICAL PROPERTIES OF LOW SULPHUR STEEL |
| HU Hanqi;ZHENG Riqi University of Science and Technology Beijing professor;Faculty of Casting;University of Science and Technology Beijing;Beijing 100083 |
引用本文:
胡汉起;郑日琪. 电磁搅拌对低硫钢枝晶组织及机械性能的影响[J]. 金属学报, 1990, 26(4): 83-86.
,
.
INFLUENCE OF ELECTROMAGNETIC STIRRING ON DENDRITIC STRUCTURE AND MECHANICAL PROPERTIES OF LOW SULPHUR STEEL[J]. Acta Metall Sin, 1990, 26(4): 83-86.
1 Junze J, Kobayashi K F, Shingu P H. Metall Trans, 1984; 15A: 307 2 Stein D. Trans Am Foundrymen's Soc, 1980; 88: 631 3 北京钢铁学院,东北工学院编.工程力学,中册,第一分册,北京:人民教育出版社,1981:174 4 Ohno A. The Solidification of Metals, Tokyo. Chijin Shokan Co., 1967: 112 5 胡汉起,钟雪友,韩青有.金属学报,1987;23:A176 6 Feuervacher B, Hamacher H. Materials Science in Space, Berlin: Springer-Verlag, 1986: 122" |
|