| Fe-Mn-C合金奥氏体强化对马氏体相变的影响 |
| 潘牧;徐祖耀 |
| 上海交通大学;上海交通大学材料科学系;教授;上海(200030) |
|
| INFLUENCE OF AUSTENITE STRENGTHENING ON MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS |
| PAN Mu;XU Zuyao T. Y. Hsu Shanghai Jiao Tong University XU Zuyao; professor; Dept. of Materials Science; Shanghai Jiao Tong University;Huashan Road; Shanghai 200030 China |
引用本文:
潘牧;徐祖耀. Fe-Mn-C合金奥氏体强化对马氏体相变的影响[J]. 金属学报, 1989, 25(6): 5-9.
,
.
INFLUENCE OF AUSTENITE STRENGTHENING ON MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS[J]. Acta Metall Sin, 1989, 25(6): 5-9.
1 Nichol T J, Judd G, Ansell G S. Metall Trans, 1977; 8A: 1877 2 Hsu T Y (徐祖耀), Li Jian (李箭), Zeng Zhenpeng (曾振鹏), Metallography, 1986; 19: 305 3 Hsu T Y (徐祖耀), Chen Weichong (陈卫中). Scr Metall, 1987; 21: 1289 4 Thomas G. Metall Trans, 1971; 2A: 2373 S Kung C Y, Rayment J J. Metall Trans, 1982; 13A: 328 6 徐祖耀,金属学报,1979;15:329 7 Haasen P. In: Nabarro F R N ed, Dislocation in Solids, Vol. 4, Dislocations in Metallurgy, Amsterdan: North-Holland, 1979: 155 8 Huang D, Thomas G, Metall Trans, 1971; 2A: 1587 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|