| 动态应变时效对奥氏体不锈钢纯弯疲劳强度的影响 |
| 陈文哲;钱匡武 |
| 福州大学机械系;讲师;福州市;福州大学 |
|
| EFFECTS OF DYNAMIC STRAIN AGING ON PURE BENDING FATIGUE STRENGTH OF AUSTENITIC STAINLESS STEEL |
| CHEN Wenzhe;QIAN Kuangwu Fuzhou University |
引用本文:
陈文哲;钱匡武. 动态应变时效对奥氏体不锈钢纯弯疲劳强度的影响[J]. 金属学报, 1989, 25(2): 56-60.
,
.
EFFECTS OF DYNAMIC STRAIN AGING ON PURE BENDING FATIGUE STRENGTH OF AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 1989, 25(2): 56-60.
1 Qian K W (钱匡武), Ni C F (倪潮方). Proc 5th Int Conf on Heat Treatment of Materials, Vol. Ⅰ, Oct. 20--24, 1986, Budapest, Hungary, 1986: 592 2 陈文哲.福州大学硕士论文,1987 3 陈文哲,钱匡武.DSA对奥氏体不锈钢静拉伸强度的影响,待发表 4 胡庚祥,钱苗根.金属学,上海科技出版社,1980:290 5 赵敬世.位错理论基础,北京航空学院,1982:146 6 肖纪美,不锈钢的金属学问题,冶金工业出版社,1983:39z |
|