| SiC_w/Al复合材料的微观结构与性能 |
| 郭树启;韩圭焕;姚忠凯 |
| 哈尔滨工业大学;沈阳中国科学院金属研究所;哈尔滨工业大学;哈尔滨工业大学;617信箱 |
|
| MICROSTRUCTURES AND PROPERTIES OF SiC_w/Al COMPOSITES |
| GUO Shuqi;HAN Guihuan;YAO Zhongkai Harbin Institute of Technology |
引用本文:
郭树启;韩圭焕;姚忠凯. SiC_w/Al复合材料的微观结构与性能[J]. 金属学报, 1988, 24(6): 499-504.
,
,
.
MICROSTRUCTURES AND PROPERTIES OF SiC_w/Al COMPOSITES[J]. Acta Metall Sin, 1988, 24(6): 499-504.
1 McDanels D L, Hoffman C A. NASA-TM-83610, 1982 2 Starke E A Jr., Sanders T H Jr., Palmer I G. J Met, 1981; 33: 24 3 Divecha A P, Fishman S G. In: Miller K J, Smith R F eds., Machanical Behavior of Materials, Vol. Ⅲ, Proc 3rd Int Conf on Machanical Behavior of Materials, Cambridge, Aug, 20--24, 1979, Oxford: Pergamon, 1980: 351 4 Nieh T G, Rainen R A, Chellman D J, In: Harrigan W C Jr., Strife J, Dhingra A K eds., Proc 5th Int Conf on Composites Materials, ICCM/2, San Diego Califonia, USA, 29--30 July, 1 Aug., 1985, Warrendale: Metallutgical Society of AIME, 1985: 825 5 Sakamoto A, Hasegawa H, Minoda Y. In: Harrigan W C Jr., Strife J, Dhingra A K. eds. Proc 5th Int Conf on Composites Materials, ICCM/2, San Diego Califonia, USA, 29--30 July. 1 Aug., 1985, Warrendale: Metallutgical Society of AIME, 1985: 699 6 Phillips W L. Proc of the 1978 Int Conf on Composites Materials ICCM/2, Toronto, Canada, Apr. 16--20, 1978, Warrendale: Metallutgical Society of AIME, 1978: 567 7 Parrat N J. Fiber Reinforced Materials Technology, London, U. K.: Van Nostrand-Reinhold, 1972: 159 8 郭树启,曹利,韩圭焕,姚忠凯.复合材料学报,1987;4(3) :32 9 Nutt S R. J Am Ceram Soc, 1984; 67 (6) : 428 10 堂,本忠,立松义明,田中淳夫.日本公开特许.昭59-70736,1984:179% |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|