| Fe_(70)Cr_(18)Mo_2Si_1B_9单辊激冷带中的特殊结晶现象 |
| 林一坚;尤云龙;张小岷;井春永;郁泉琴 |
| 上海昊淞上海钢铁研究所;上海钢铁研究所;上海钢铁研究所;上海钢铁研究所;上海钢铁研究所 |
|
| UNUSUAL SOLIDIFICATION MICROSTRUCTURE OF Fe_(70)Cr_(18)Mo_2Si_1B_9 SINGLE-ROLL QUENCHED RIBBON |
| LIN Yijian;YOU Yunlong;ZHANG Xiaomin;JING Chunyong;YU Quanqin Shanghai Iron and Steel Research Institute |
引用本文:
林一坚;尤云龙;张小岷;井春永;郁泉琴. Fe_(70)Cr_(18)Mo_2Si_1B_9单辊激冷带中的特殊结晶现象[J]. 金属学报, 1988, 24(6): 487-493.
,
,
,
,
.
UNUSUAL SOLIDIFICATION MICROSTRUCTURE OF Fe_(70)Cr_(18)Mo_2Si_1B_9 SINGLE-ROLL QUENCHED RIBBON[J]. Acta Metall Sin, 1988, 24(6): 487-493.
1 Ray R. Mater Sci Eng, 1982; 52: 85 2 Koster U, Herold U. In: Masumoto T et al. eds., Proc 4th Int Conf on the Rapidly Quenched Metals, Sendai, 1981, Japan: The Japan Institute Metals, 1982: 717 3 林一坚,尤云龙,张小岷,井春永,严守平,章靖国.金属学报,1987;23:A326 4 Kunimasa Takeshita, Paul Hideo Shingu. Trans Jpn Inst Met, 1983; 24: 529 5 Kunimasa Takeshita, Paul Hideo Shingu. Trans Jpn Inst Met, 1986; 27: 141 6 Hideo Shingu P, Kobayashi K, Sukuki R, Takashita K. In: Masumoto T et al eds., Proc 4th Int Conf on the Rapidly Quenched Metals, Sendai, 1981, Japan: The Japan Institute Metals, 1982: 57 7 Neumann W, Leonhardt M, Loser W, Sellger R, Jurisch M. J Mater Sci, 1985; 20; 3141 8 胡坚,许嘉龙,张士勋,章靖国.上海钢铁研究所硕士论文,1987 9 胡汉起.金属凝固,冶金工业出版社,1985 10 Bergmann H W, Fritsch H U. Met Sci, 1982; 16: 197 11 Kemeny T, Vincze I, Fogarassy B. Phys Rev B, 1979; 20: 476 12 Vincze I, Boudreaux D S, Tegze M. Phys Rev B, 1979; 19: 4896 13 长田和雄,井野博满.日本金属学会志,1985;49:402 |
|