| 时效对Mn-Cu-Al三元合金的内耗、杨氏模量和力学性能的影响 |
| 衣虎春;葛庭燧 |
| 中国科学院固体物理研究所;教授;合肥中国科学院固体物理研究所 |
|
| EFFECT OF AGING ON INTERNAL FRICTION, ELASTIC MODULUS AND MECHANICAL PROPERTIES OF TERNARY Mn-Cu-Al ALLOYS |
| YI Huchun;GE Tingsui (T. S. Ke) Institute of Solid State Physics; Academia Sinica. Hefei |
引用本文:
衣虎春;葛庭燧. 时效对Mn-Cu-Al三元合金的内耗、杨氏模量和力学性能的影响[J]. 金属学报, 1988, 24(5): 317-324.
,
.
EFFECT OF AGING ON INTERNAL FRICTION, ELASTIC MODULUS AND MECHANICAL PROPERTIES OF TERNARY Mn-Cu-Al ALLOYS[J]. Acta Metall Sin, 1988, 24(5): 317-324.
1 Butler E P, Kelly P M. Trans Metall Soc AIME, 1968; 242: 2099 2 Vitek J M, Warlimont H. Met Sci, 1976; 10: 7 3 Birchon D, Bromley D E, Healey D. Met Sci J, 1968; 2: 41 4 盛宗毅,私人消息 5 Sugimoto K. Mori T, Shiode S. Met Sci J, 1973; 7: 103 6 Vintaykin Ye Z, Dmitriyev V B, Udovenko V A. Phys Met Metallogr, (Eng. ed.), 1979: 44: 107 7 Smith J H, Vance E R. J Appl Phys, 1969; 40: 4853 8 Worrell F T. J Appl Phys, 1948; 19: 929 9 Zener C. Elasticity and Anelasticity of Metals, University Chicago Press, 1948: 160w |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|