| 用正电子湮没方法探讨Fe-Al合金的热处理工艺 |
| 王景成;刘大均 |
| 上海钢铁研究所测试中心;上海钢铁研究所 |
|
| POSITRON ANNIHILATION STUDY OF HEAT TREATMENT PROCESS IN Fe-22 at.-% Al |
| WANG Jingcheng;LIU Dajun Shanghai Iron and Steel Research Institute |
引用本文:
王景成;刘大均. 用正电子湮没方法探讨Fe-Al合金的热处理工艺[J]. 金属学报, 1988, 24(2): 221-222.
,
.
POSITRON ANNIHILATION STUDY OF HEAT TREATMENT PROCESS IN Fe-22 at.-% Al[J]. Acta Metall Sin, 1988, 24(2): 221-222.
1 Bergersen B, Stott M I. Solid State Commun 969; 7: 1208 2 Oki K, Hasaka M, Eguchi T. Jpn J Appl Phys, 1973; 12: 1522 3 Liu Dajun. J Magn Magn Mater, 1982; 26: 217 4 山中和夫,井野博满.日本金属学会志,1971;35,(6) :566 |
|