| 一种计算氢扩散系数的新方法 |
| 杨柯;冼爱平;曹名洲;万晓景 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;上海工业大学 |
|
| AN IMPROVED METHOD FOR CALCULATING DIFFUSIVITY OF HYDROGEN |
| YANG Ke Insittute of Metal rescarch;Academia Sinica;Shenyang;XIAN Aiping;CAO Mingzhou;WAN Xiaojing Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
杨柯;冼爱平;曹名洲;万晓景. 一种计算氢扩散系数的新方法[J]. 金属学报, 1988, 24(2): 218-220.
,
,
,
.
AN IMPROVED METHOD FOR CALCULATING DIFFUSIVITY OF HYDROGEN[J]. Acta Metall Sin, 1988, 24(2): 218-220.
1 Devanathan M A V, Stachurski Z. Proc R Soc, 1962; A270: 90 2 Chaudhari B S, Radhakrishnan T P. Surf Tech, 1984; 22; 353 3 山川宏二,鹤田孝雄,吉沢四郎.防食技术,1981;30:443 4 Beck W, Bockris J O'M, McBreen J, Naris L. Proc R Soc, 1966; A290: 220 5 Hagi H. Hayashi Y, Ohtani N. Trans Jpn Inst Met, 1979; 20: 349 6 Asano S. Hara K, Nakai Y. Ohtani N. J Jpn Inst Met, 1974; 38: 626 7 Nagano M, Hayashi Y, Ohtani N, Isshiki M, gaki K. Trans Jpn Inst Met, 1981; 22: 423 8 Nagano M, Hayashi Y, Ohtani N, Isshiki M, Igaki K. Scr Metall. 1982; 16: 973 9 Gibala R. Trans Metall Soc AIME. 1967; 239: 1574 10 Bernstem I M. Scr Metall, 1974; 8: 343 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|