    					| Ti和V对Fe中氢与位错交互作用的影响 | 
  					 
  					  										
						| 毛鸥;杜家驹 | 
					 
															
					| 中国科学院固体物理研究所;中国科学院固体物理研究所;副研究员;合肥 | 
					 
										
						 | 
					 
   										
    					| EFFECT OF Ti AND V ON HYDROGEN-DISLOCATION INTERACTION IN Fe | 
  					 
  					  					  					
						| MAO Ou Institute of Solid State Physics;Academia Sinica; HefeiDU Jiaju Associate Professor;Institute of Solid State Physics;Academia Sinica Hefei | 
					 
														 
				
				引用本文: 
				
								毛鸥;杜家驹. Ti和V对Fe中氢与位错交互作用的影响[J]. 金属学报, 1988, 24(1): 11-16.	
																												 																				 ,
																												 . 
				EFFECT OF Ti AND V ON HYDROGEN-DISLOCATION INTERACTION IN Fe[J]. Acta Metall Sin, 1988, 24(1): 11-16.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  1 Donovan J A. Metall Trans, 1976; 7A: 1677 2 Fujita F E. Trans Jpn Inst Met, 1976; 17: 232 3 Heller W R. Acta Metall, 1961; 9: 600 4 Gibala R. Trans AIME, 1967; 239: 1574 5 Weiner L C, Gensamer M. Acta Metall, 1957; 5: 692 6 Asano S, Kitamura A, Otsuka R. Scr Metall. 1978; 12: 805 7 Kikuta Y, Sugimoto K, Ochiai S, Iwata K. Trans Iron Steel Inst Jpn. 1975; 15: 87 8 Ritchie I G, Dufresne J F, Moser P. Phys Status Solidi, 1979; 52A: 331 9 Sturges C M. Miodownik A P. Acta Metall, 1969; 17: 1197 10 Du J J, Mao O, Wang X. In: Yan M G et al eds., Mechanical Behaviour of Materials-V, New York: Pergamon, 1987; 855 11 Shirley A I, Hall CK. Scr Metall, 1983; 17: 1003 12 Koiwa M. Acta Metoll, 1974; 22: 1259 13 Hirth J P. Metall Trans. 1980; 11A: 861 14 Schoeck G. Acta Metall, 1963; 11: 617 15 Seeger A. Phys Status Solidi. 1979; 55A: 457H | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |