| Cu-Bi合金偏析的原子模拟 Ⅱ.偏析引起的晶界结构转变 |
| 王桂金;V.VITEK |
| 冶金工业部钢铁研究总院6室;高级工程师;北京西直门外;美国宾夕法尼亚大学 |
|
| ATOMISTIC SIMULATION OF SEGREGATION IN Cu-Bi SYSTEM II. SEGREGATION INDUCED STRUCTURAL TRANSFORMATIONS AT GRAIN BOUNDARIES |
| WANG Guijin Senior engineer;Central Iron and Steel Reseorch Institute;Ministry of Metatturgicol Industry;Beijing;V. VITEK Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing;V. VITEK Central Iron and steel Research Institute; Ministry of Metallurgical Industry. Beijing; University of Pennsylvania; USA |
引用本文:
王桂金;V.VITEK. Cu-Bi合金偏析的原子模拟 Ⅱ.偏析引起的晶界结构转变[J]. 金属学报, 1988, 24(1): 6-10.
,
.
ATOMISTIC SIMULATION OF SEGREGATION IN Cu-Bi SYSTEM II. SEGREGATION INDUCED STRUCTURAL TRANSFORMATIONS AT GRAIN BOUNDARIES[J]. Acta Metall Sin, 1988, 24(1): 6-10.
1 Hart E W. In: Hu Hsun ed., Nature and Behavior of Grain Boundaries, New York: Plenum Ptess, 1972: 155 2 Aust K T. Can Met Q, 1969; 8: 173 3 Wang G J. Ph D thesis, 1984, University of Pennsylvania 4 Wang G J. Sutton A P, Vitek Y. Acta Metall, 1984; 32: 1093 5 Vitek V, Minonishi Y, Wang G J. J Phys (Paris), 1985; 46: C4--171 6 Hashimoto M, Ishida Y, Yamamoto R, Doyama M. Fujiwara T. Scr Metall, 1982; 16: 267 7 Hashimoto M, Ishida Y, Yamamoto R, Doyama M. Acte Metall, 1984; 32: 1 8 Vitek V, Wang G J. Surf Sci, 1984; 144: 110 9 King A H. Acta Metall, 1982; 30: 419 |
|