稀土镁合金微细电火花加工变质层微观结构及性能研究 |
孙术发1, 2),狄士春1),吕鹏翔1),韦东波1),喻杰1),郭豫鹏1) |
1) 哈尔滨工业大学机电工程学院, 哈尔滨 150001
2) 东北林业大学工程技术学院, 哈尔滨 150040 |
|
MICROSTRUCTURE AND PROPERTIES OF METAMORPHIC LAYER FORMED ON Mg-RE ALLOY IN MICRO-EDM PROCESS |
SUN Shufa 1, 2), DI Shichun 1), LU Pengxiang 1), WEI Dongbo 1),YU Jie 1), GUO Yupeng 1) |
1) School of Mechatronics Engineering, Harbin Institute of Technology, Harbin 15000
12) Institute of Engineering and Technology, Northeast Forestry University, Harbin 150040 |
引用本文:
孙术发,狄士春,吕鹏翔,韦东波,喻杰,郭豫鹏. 稀土镁合金微细电火花加工变质层微观结构及性能研究[J]. 金属学报, 2013, 49(2): 251-256.
SUN Shufa,
DI Shichun,
LU Pengxiang,
WEI Dongbo,
YU Jie,
GUO Yupeng.
MICROSTRUCTURE AND PROPERTIES OF METAMORPHIC LAYER FORMED ON Mg-RE ALLOY IN MICRO-EDM PROCESS[J]. Acta Metall Sin, 2013, 49(2): 251-256.
[1] Yao H B, Li Y, Wee A T S. Electrochim Acta, 2003; 48: 4197
[2] Chen H B, Yang B. Int J Min Met Mater, 2009; 16: 672
[3] Wang X B, Tian X B, Gong C Z, Yang S Q. J Inorg Mater, 2011; 26: 711
(王晓波, 田修波, 巩春志, 杨士勤. 无机材料学报, 2011; 26: 711)
[4] Ding W J, Zeng X Q. Acta Metall Sin, 2010; 46: 1450
(丁文江, 曾小勤. 金属学报, 2010; 46: 1450)
[5] Li H Z, Liu H T, Li F B, Wang H J, Liang X P, Liu C M. J Mater Eng Perform, 2012; 21: 1056
[6] Chang J W, Guo X W, He S M, Fu P H, Peng L M, Ding W J. Corros Sci, 2008; 50: 166
[7] Chang J W, Duo J, Xiang Y Z, Yang H Y, Ding W J, Peng Y H. Int J Min Met Mater, 2011; 18: 203
[8] Peng L M, Chang J W, Guo X W, Atrens A, Ding W J, Peng Y H. J Appl Electrochem, 2009; 39: 913
[9] Xu N J, Liu C S, Shang S, Wang Z Y. J Northeastern Univ (Nat Sci), 2012; 33: 1133
(许妮君, 刘常升, 商硕, 王政一. 东北大学学报(自然科学版), 2012; 33: 1133)
[10] Guckel H, Fischer K, Stiers E, Chaudhuri B, McNamara S, Ramotowski M, Johnson E D, Kirk C. Microsyst Technol, 1999; 6: 103
[11] Liu J C, Bai J C, Guo Y F. Non-Traditional Machining Technology.5th Ed., Beijing: China Machine Press, 2010: 7
(刘晋春, 白基成, 郭永丰. 特种加工. 第5版. 北京:机械工业出版社, 2010: 7)
[12] Osenbruggen C V. Philips Technish Tijdschrift, 1969; 20: 200
[13] Joo C P, Kim B H, Choi D K, Chu C N. J Mech Sci Technol, 2008; 22: 300
[14] Ghanem F, Braham C, Sidhom H. J Mater Process Technol, 2003; 142: 163
[15] Cho D H, Lee S A, Lee Y Z. Tribology Lett, 2012; 45: 123
[16] Ma G R, Xu Z J. Electromachining, 1984; 3: 5
(马光荣, 徐祯基. 电加工, 1984; 3: 5)
[17] Zhao W S. Advanced EDM Machining Technology. Beijing: National Defence Industry Press, 2003: 34
(赵万生. 先进电火花加工技术. 北京: 国防工业出版社, 2003: 34)
[18] Jahan M P, Wong Y S, Rahman M. J Mater Process Technol, 2009; 209: 1706
[19] Bouvier Y, Mutel B, Grimblot J. Surf Coat Technol, 2004; 18: 169
[20] Kumar S, Singh R, Singh T P, Sethi B L. J Mater Process Technol, 2009; 209: 3675
[21] Harcuba P, Bacakova L, Strasky J, Bacakova M, Novotna K, Janecek M. J Mech Behav Biomed Mater, 2012; 7: 96
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|