| 超大热输入焊接用EH40钢的模拟熔合线组织与性能 |
| 张朋彦, 高彩茹, 朱伏先 |
| 东北大学 轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| MICROSMICROSTRUCTURE AND MECHANICAL PROPERTIES OF SIMULATE FUSION LINE IN EH40 SHIP PLATE STEEL FOR HIGH HEAT INPUT WELDING |
| ZHANG Pengyan, GAO Cairu, ZHU Fuxian |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
|
引用本文:
张朋彦 高彩茹 朱伏先. 超大热输入焊接用EH40钢的模拟熔合线组织与性能[J]. 金属学报, 2012, 48(3): 264-270.
,
,
.
MICROSMICROSTRUCTURE AND MECHANICAL PROPERTIES OF SIMULATE FUSION LINE IN EH40 SHIP PLATE STEEL FOR HIGH HEAT INPUT WELDING[J]. Acta Metall Sin, 2012, 48(3): 264-270.
| [1] Zhang H Q, Jiang L Z. Baosteel Technol, 2006; 4: 20(张汉谦, 江来珠. 宝钢技术, 2006; 4: 20)[2] Mi G S, Chen D Z, Qu F. Pet Chem Constr, 2009; 29(5): 25(米广生, 陈德志, 瞿 帆. 石油化工建设, 2009; 29(5): 25)[3] Luo X B, Su H, Yang C F, Chai F, Yuan X M. Trans China Weld Inst, 2010; 31(10): 57(罗小兵, 苏航, 杨才福, 柴锋, 袁晓敏. 焊接学报, 2010; 31(10): 57)[4] Suzuki S, Ichimiya K, Akita T. JFE Tech Rep, 2004; 5: 19[5] Hitoshi H. Tetsu Hagane, 2004; 5: 271[6] Minagawa M, Ishikawa T, Mabuchi H. CAMP–ISIJ, 1997; 10: 590[7] Hong S G, Kang K J, Park C G. Scr Mater, 2002; 6: 163[8] Vega M I, Medina S F, Quispe A, Gomez M, Gomez P P. ISIJ Int, 2005; 45: 1878[9] Kasamatsu Y. Tetsu Hagane, 1979; 65: 1232[10] Kojima A, Kiyose A, Minagawa M, Hirano A, Yoshii K, Nakajima T, Hoshino M, Ueshima Y. CAMP–ISIJ, 2003; 16: 360[11] Kiyomichi N, Akihiro Y, Sengo K, Masahiko H, Yuichi K. Tetsu Hagane, 2004; 90: 141[12] Qiu P J, Michihiko N. Tetsu Hagane, 1998; 84: 592[13] Matsuda S, Okumura N, Okamura Y. Tetsu Hagane, 1974; 60: 174[14] Matsuda S, Okumura N. Tetsu Hagane, 1976; 62: 1209[15] Kasamatsu Y, Takashima S, Hosoya T. Tetsu Hagane, 1976; 62: 678[16] Mukae S, Nishio K, Katoh M, Isayama T. PJWS, 1985; 3(3): 131[17] Koda M, Amano K, Funahashi Y, Shiga C, Ueda S. Tetsu Hagane, 1984; 70: 1265[18] ShuW, Wang X M, Li S R, He X L. Acta Metall Sin, 2011; 47: 435(舒玮, 王学敏, 李书瑞, 贺信莱. 金属学报, 2011; 47: 435)[19] Han S C. Dev Appl Mater, 1995; 10: 2[20] Murakani T, Takeda H, Nanba S. PJWS, 2004; 75: 324[21] Kang Y B, Lee H G. ISIJ Int, 2010; 50: 501[22] Yamamoto K, Jinichi T. ISIJ, 1996; 36: 80[23] Shim J, Cho Y. Acta Mater, 1999; 47: 2751[24] Ishikawa F, Takahashi F. ISIJ, 1995; 35: 1128[25] Madariaga I, Gutierrez I. Acta Mater, 1999; 47: 95[26] Enomoto M. Met Mater Int, 1998; 4: 115[27] Lee J L. Acta Metall Mater, 1994; 42: 3291[28] Pan Y T, Lee J L. Mater Des, 1994; 15: 331[29] Hong S G, Kang K J, Park C G. Scr Mater, 2002; 6: 163[30] Yamamoto K, Hasegawa T, Takamura J. ISIJ, 1996; 36: 80[31] Jinichi T, Shozo M. Proceedings of the Sixth Internal Iron and Steel Congress. Nagoya: Iron and Steel Institute of Japan, 1999: 591 |
|