镍基单晶高温合金冷热循环过程中圆孔周围裂纹萌生与扩展行为 |
王莉1( ),周忠娇1,张少华1sup,降向冬2,楼琅洪1,张健1 |
2 北京北冶功能材料有限公司, 北京 100192 |
|
CRACK INITIATION AND PROPAGATION AROUND HOLES OF Ni-BASED SINGLE CRYSTAL SUPERALLOY DURING THERMAL FATIGUE CYCLE |
Li WANG1( ),Zhongjiao ZHOU1,Shaohua ZHANG1,Xiangdong JIANG2,Langhong LOU1,Jian ZHANG1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2 Beijing Beiye Functional Materials Corporation, Beijing 100192 |
引用本文:
王莉,周忠娇,张少华,降向冬,楼琅洪,张健. 镍基单晶高温合金冷热循环过程中圆孔周围裂纹萌生与扩展行为[J]. 金属学报, 2015, 51(10): 1273-1278.
Li WANG,
Zhongjiao ZHOU,
Shaohua ZHANG,
Xiangdong JIANG,
Langhong LOU,
Jian ZHANG.
CRACK INITIATION AND PROPAGATION AROUND HOLES OF Ni-BASED SINGLE CRYSTAL SUPERALLOY DURING THERMAL FATIGUE CYCLE[J]. Acta Metall Sin, 2015, 51(10): 1273-1278.
[1] | He G, Li J G, Mao X M, Fu H Z. Mater Rev, 1994; (1): 12 (何 国, 李建国, 毛协民, 傅恒志. 材料导报, 1994; (1): 12) | [2] | Yue Z F, Yin Z Y, Yang Z G. Aeroengine, 1997; (4): 32 (岳珠峰, 尹泽勇, 杨治国. 航空发动机, 1997; (4): 32) | [3] | Ohyszko A, Kubiak K, Sieniawski J. J Achievements Mater Manuf Eng, 2009; 32(1): 66 | [4] | Shah D M, Cetel A. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Warrendale: TMS, 2000: 295 | [5] | Duhl D N, Cetel A D. US Pat, 4719080, 1988 | [6] | Harris K, Wahl J B. In: Strang A, Banks W M, Conroy R D, McColvin, Neal J C, Simpson S eds., Proc 5th Int Charles Parsons Turbine Conf, London: Cambridge University, 2000: 832 | [7] | Walston W S, O'hara K S, Ross E W, Pollock T M, Murphy W H. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale: TMS, 1996: 27 | [8] | Fuchs G E. J Mater Eng Perform, 2002; 11(1): 19 | [9] | Hollwarth B R, Dagan L. ASME J Eng Power, 1980; 102: 994 | [10] | McNally C A, Folkes J, Pashby I R. Mater Sci Technol, 2004; 20: 805 | [11] | Kim Y J, Kim S M. Int J Heat Mass Transfer, 2004; 47: 245 | [12] | Hou N X, Wen Z X, Du Z X, Yue Z F. Theor Appl Fract Mech, 2007; 47: 164 | [13] | Das D K, Pollock T M. J Mater Proc Technol, 2009; 209: 5661 | [14] | Zhou Z J, Wang L, Wen J L, Lou L H, Zhang J. J Alloys Compd, 2015; 628: 158 | [15] | Wang J L, Chen M H, Yang L L, Zhu S L, Wang F H. Corros Sci, 2015; 98: 530 | [16] | Alamn M Z, Satyanarayana D V V, Chatterjee D, Sarkar R, Das D K. Mater Sci Eng, 2015; A641: 84 | [17] | Wang L, Zhou Z J, Jiang W G, Wang D, Shen J, Lou L H. Chin J Mater Res, 2014; 28: 663 (王 莉, 周忠娇, 姜卫国, 王 迪, 申 健, 楼琅洪. 材料研究学报, 2014; 28: 663) | [18] | Sabnis P A, Maziere M, Forest S, Arakere N K, Ebrahimi F. Int J Plast, 2012; 28: 102 | [19] | Li Y L, Yuan C, Guo J T. Acta Metall Sin, 2006; 42: 1056 (李友林, 袁 超, 郭建亭. 金属学报, 2006; 42: 1056) | [20] | Xia P C, Yu J J, Sun X F, Guan H R, Hu Z Q. Rare Met Mater Eng, 2008; 37: 50 (夏鹏成, 于金江, 孙晓峰, 管恒荣, 胡壮麒. 稀有金属材料与工程, 2008; 37: 50) | [21] | Liu Y, Yu J J, Xu Y, Sun X F. Rare Met Mater Eng, 2009; 38: 59 (刘 源, 于金江, 徐 岩, 孙晓峰. 稀有金属材料与工程, 2009; 38: 59) | [22] | Xiao X, Xu H, Qin X Z, Guo Y A, Guo J T, Zhou L Z. Acta Metall Sin, 2011; 47: 1129 (肖 旋, 许 辉, 秦学智, 郭永安, 郭建亭, 周兰章. 金属学报, 2011; 47: 1129) | [23] | Liu J L, Jin T, Zhang J H, Hu Z Q. Acta Metall Sin, 2001; 37: 1233 (刘金来, 金 涛, 张静华, 胡壮麒. 金属学报, 2001; 37: 1233) | [24] | Zhao N R, Wang Z H, Li J G, Jin T, Sun X F, Yang H C, Hu Z Q. J Mater Eng, 2008; (2): 58 (赵乃仁, 王志辉, 李金国, 金 涛, 孙晓峰, 杨洪才, 胡壮麒. 材料工程, 2008; (2): 58) | [25] | Li J R, Shi Z X, Yuan H L, Liu S Z, Zhao J Q, Han M, Liu W W. J Mater Eng, 2008; (12): 6 (李嘉荣, 史振学, 袁海龙, 刘世忠, 赵金乾, 韩 梅, 刘维维. 材料工程, 2008; (12): 6) | [26] | Jia Y X, Jin T, Liu J L, Sun X F, Hu Z Q. Acta Metall Sin, 2009; 45: 1364 (贾玉贤, 金 涛, 刘金来, 孙晓峰, 胡壮麒. 金属学报, 2009; 45: 1364) | [27] | Hu G X,Cai X,Rong Y H. Fundamentals of Materials Science. 3rd Ed., Shanghai: Shanghai Jiaotong University Press, 2010: 431 (胡赓祥,蔡 珣,戎咏华. 材料科学基础 (第三版). 上海: 上海交通大学出版社, 2010: 431) | [28] | Jin Z X. Central Iron Steel Res Inst Tech Bull, 1985; 5: 205 (金哲学. 钢铁研究总院学报, 1985; 5: 205) | [29] | Academic Committee of the Superalloys,The Chinese Society for Metals. China Superalloys Handbook. Beijing: Standards Press of China, 2012 (中国金属学会高温材料分会编. 中国高温合金手册. 北京: 中国标准出版社, 2012) | [30] | Chao J, Gonzalez-Carrasco J L. Mater Sci Eng, 1997; A230: 39 |
|
|