球墨铸铁凝固显微组织的元胞自动机模拟* |
张蕾, 赵红蕾, 朱鸣芳( ) |
东南大学江苏省先进金属材料高技术研究重点实验室, 南京 211189 |
|
SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD |
ZHANG Lei, ZHAO Honglei, ZHU Mingfang( ) |
Jiangsu Key Laboratory for Advanced Metallic Materials, Southeast University, Nanjing 211189 |
引用本文:
张蕾, 赵红蕾, 朱鸣芳. 球墨铸铁凝固显微组织的元胞自动机模拟*[J]. 金属学报, 2015, 51(2): 148-158.
Lei ZHANG,
Honglei ZHAO,
Mingfang ZHU.
SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD[J]. Acta Metall Sin, 2015, 51(2): 148-158.
[1] |
Lei F J. Hot Working Technol, 2008; 37(13): 125
|
[1] |
(雷富军. 热加工工艺, 2008; 37(13): 125)
|
[2] |
Zhou J Y. Color Metallography of Cast Irons. Beijing: China Machine Press, 2002: 98
|
[2] |
(周继扬. 铸铁彩色金相学. 北京: 机械工业出版社, 2002: 98)
|
[3] |
Shi Y F, Xu Q Y, Gong M, Liu B C. Acta Metall Sin, 2011; 47: 620
|
[3] |
(石玉峰, 许庆彦, 龚 铭, 柳百成. 金属学报, 2011; 47: 620)
|
[4] |
Wu M W, Xiong S M. Acta Metall Sin, 2010; 46: 1534
|
[4] |
(吴孟武, 熊守美. 金属学报, 2010; 46: 1534)
|
[5] |
Jiang H X, Zhao J Z. Acta Metall Sin, 2011; 47: 1099
|
[5] |
(江鸿翔, 赵九洲. 金属学报, 2011; 47: 1099)
|
[6] |
Zhang X F, Zhao J Z. Acta Metall Sin, 2012; 48: 615
|
[6] |
(张显飞, 赵九洲. 金属学报, 2012; 48: 615)
|
[7] |
Dai T, Zhu M F, Chen S L, Cao W S, Hong C P. Acta Metall Sin, 2008; 44: 1175
|
[7] |
(戴 挺, 朱鸣芳, 陈双林, 曹伟生, 洪俊杓. 金属学报, 2008; 44: 1175)
|
[8] |
Yang Z R, Sun D K, Pan S Y, Dai T, Zhu M F. Acta Metall Sin, 2009; 45: 43
|
[8] |
(杨朝蓉, 孙东科, 潘诗琰, 戴 挺, 朱鸣芳. 金属学报, 2009; 45: 43)
|
[9] |
Li Z Y, Zhu M F, Dai T. Acta Metall Sin, 2013; 49: 1032
|
[9] |
(李正扬, 朱鸣芳, 戴 挺. 金属学报, 2013; 49: 1032)
|
[10] |
Charbon C, Rappaz M. In: Lesoult G, Lacaze J eds., Physical Metallurgy of Cast Iron V. Switzerland: Scitec Publications, 1997: 453
|
[11] |
Ruxanda R, Beltran-Sanchez L, Massone J, Stefanescu D M. Trans AFS, 2001; 109: 1037
|
[12] |
Gurgul D, Burbelko A. Arch Metall Mater, 2010; 55: 53
|
[13] |
Burbelko A, Fras E, Gurgul D, Kapturkiewicz W, Sikora J. Key Eng Mater, 2011; 457: 330
|
[14] |
Burbelko A A, Gurgul D, Kapturkiewic W, Górny M. Mater Sci Eng, 2012; 33: 012083
|
[15] |
Zhao H L, Zhu M F, Stefanescu D M. Key Eng Mater, 2011; 457: 324
|
[16] |
Zhu M F, Pan S Y, Sun D K, Zhao H L. ISIJ Int, 2010; 50: 1851
|
[17] |
Zhu M F, Stefanescu D M. Acta Mater, 2007; 55: 1741
|
[18] |
Stefanescu D M. Science and Engineering of Casting Solidification. 2nd Ed., New York: Springer, 2009: 220
|
[19] |
Zhu M, Zhang L, Zhao H, Stefanescu D M. Acta Mater, 2015; 84: 413
|
[20] |
Brown S G R, Williams T, Spittle J A. Acta Metall Mater, 1994; 42: 2893
|
[21] |
Stefanescu D M, Katz S. In: Vishwanatan S ed., ASM Handbook. Vol.15, Materials Park, Ohio: ASM International, 2008: 41
|
[22] |
Zheng H L, Sun Y C, Zhang N, Tian X L. ISIJ Int, 2010; 50: 1981
|
[23] |
Pedersen K M, Tiedje N S. Mater Charact, 2008; 59: 1111
|
[24] |
Torres J F L. PhD Dissertation, University of Alabama, Tuscaloosa, America, 2003
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|