钛铝金属间化合物的进展与挑战* |
杨锐( ) |
中国科学院金属研究所, 沈阳 110016 |
|
ADVANCES AND CHALLENGES OF TiAl BASE ALLOYS |
( ) |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
杨锐. 钛铝金属间化合物的进展与挑战*[J]. 金属学报, 2015, 51(2): 129-147.
.
ADVANCES AND CHALLENGES OF TiAl BASE ALLOYS[J]. Acta Metall Sin, 2015, 51(2): 129-147.
[1] |
McAndrew J B, Kessler H D. JOM, 1956; 10: 1348
|
[2] |
Shechtman D, Blackburn M J, Lipsitt H A. Metall Trans, 1974; 5: 1373
|
[3] |
Lipsitt H A, Shechtman D, Schafrik R E. Metall Trans, 1975; 6A: 1991
|
[4] |
Schuster J C, Palm M. J Phase Equilib Diffus, 2006; 27: 255
|
[5] |
Huang S C, Chesnutt J C. In: Westbrook J H, Fleischer R L eds., Structural Applications of Intermetallic Compounds. Chapter 4, New York: Wiley, 2000: 1
|
[6] |
Kainuma R, Palm M, Inden G. Intermetallics, 1994; 2: 321
|
[7] |
Ohnuma I, Fujita Y, Mitsui H, Ishikawa K, Kainuma R, Ishida K. Acta Mater, 2000; 48: 3113
|
[8] |
Suzuki A, Takeyama M, Matsuo T. Intermetallics, 2002; 10: 915
|
[9] |
Veeraraghavan D, Pilchowski U, Natarajan, B, Vasudevan V K. Acta Mater, 1998; 46: 405
|
[10] |
Witusiewicz V T, Bondar A A, Hecht U, Rex S, Velikanova T Ya. J Alloys Compd, 2008; 465: 64
|
[11] |
Blackburn M J, Smith M P. R&D on Composition and Processing of Titanium Aluminide Alloys for Turbine Engines, AFWAL-TR-82-4086, June, 1982
|
[12] |
Lipsitt H A. In: Koch C C, Liu C T, Stoloff N S eds., High-Temperature Ordered Intermetallic Alloys. Materials Research Society Symposia Procedings. Vol.39, Warrendale, PA: MRS, 1985: 351
|
[13] |
Dimiduk D M, Dutton R. Technical Report OMB No. 0704-0188, Materials and Manufacturing Directorate Air Force Research Laboratory, January, 2004
|
[14] |
National Research Council(NRC). Accelerating Technology Transition: Bridging the Valley of Death for Materials and Processes in Defense Systems. Washington: The National Academies Press, 2004: 1
|
[15] |
Aoki K, Izumi O. Nippon Kinzoku Gakkaishi, 1979; 43: 1190
|
[16] |
Liu C T, White C L, Horton J A. Acta Metall, 1985; 33: 213
|
[17] |
Djanarthany S, Viala J C, Bouix J. Mater Chem Phys, 2001; 72: 301
|
[18] |
Kim Y W, Wagner R, Yamaguchi M eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1995: 1
|
[19] |
Kim Y W. JOM, 1989; 41(7): 24
|
[20] |
Kim Y W, Dimiduk D M. JOM, 1991; 43(8): 40
|
[21] |
Kim Y W. JOM, 1994; 46(7): 30
|
[22] |
Kim Y W. JOM, 1995; 47(7): 39
|
[23] |
Larsen D E Jr. Mater Sci Eng, 1996; A213: 128
|
[24] |
National MaterialsManufacturing Board. Materials Needs and Research and Development Strategy for Future Military Aerospace Propulsion Systems. Washington: National Academies Press, 2011: 188
|
[25] |
Sadler P, Kumar K S, Green J A S. Martin Marietta Laboratories Technical Report MML-TR-93-09, 1993
|
[26] |
Pollock T M, Steif P S. A University-Industry Partnership for Research and Transition of Gamma Titanium Aluminides: Final Report, AFRL-SR-BL-TR-01-0633, 1999
|
[27] |
Draper S L, Lerch B A, Pereira M, Miyoshi K, Arya V K, Zhuang W. Durability Assessment of Gamma TiAl–Final Report, NASA/TM-2004-212303, 2004
|
[28] |
Murtagian G R. PhD Dissertation, Georgia Institute of Technology, 2004
|
[29] |
Tetsui T. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 15
|
[30] |
Wu X. Intermetallics, 2006; 14: 1114
|
[31] |
Gebauer K. Intermetallics, 2006; 14: 355
|
[32] |
European Commission DG Research and Innovation. Light-Weight Valves for High-Efficiency Engines, 2000-2004.
|
[33] |
Appel F, Paul D H, Oehring M. Gamma Titanium Aluminide Alloys: Science and Technology. Weinheim, Germany: Wiley, 2011: 1
|
[34] |
Chen G L, Sun Z Q, Zhou X. Mater Sci Eng, 1992; A153: 597
|
[35] |
Paul J D H, Appel F, Wagner R. Acta Mater, 1998; 46: 1075
|
[36] |
Xu X J, Lin J P, Zhang L Q, Liang Y F. In: Kim Y W, Smarsly W, Lin J P, Dimiduk D eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2014: 71
|
[37] |
Hu D, Huang A J, Gregoire A, Li X, Wu X, Loretto M. Mater Sci Forum, 2005; 29: 172
|
[38] |
Blackburn M J. In: Jaffee R, Promisel N eds., The Science, Technology and Applications of Titanium. London: Pergamon, 1970: 633
|
[39] |
Kumagai T, Abe E, Takeyama M, Nakamura M. Scr Mater, 1997; 36: 523
|
[40] |
Hu D, Huang A J, Novovic D, Wu X. Intermetallics, 2006; 14: 818
|
[41] |
Huang A J, Loretto M H, Hu D, Liu K, Wu X. Intermetallics, 2006; 14: 838
|
[42] |
Naka S. In: Nathal M V, Darolia R, Liu C T, Martin P L, Miracle D B, Wagner R, Yamaguchi M eds., Structural Intermetallics, Warrendale, PA: TMS, 1997: 313
|
[43] |
Burgers W G. Physica, 1934; 1: 561
|
[44] |
Kim Y W, Kim S L, Dimiduk D, Woodward C. In: Kim Y W, Morris D, Yang R, Leyens C eds., Structrural Applications for High Temperatures, Warrendale, PA: TMS, 2008: 215
|
[45] |
Clemens H, Chladil H F, Wallgram W, Zickler G A, Gerling R, Liss K D, Kremmer S, Güther V, Smarsly W. Intermetallics, 2008; 16: 827
|
[46] |
Wallgram W, Schmölzer T, Cha L M, Das G, Güther V, Clemens H. Int J Mater Res, 2009; 100: 1021
|
[47] |
Huang Z W, Cong T. Intermetallics, 2010; 18: 161
|
[48] |
Norris G. Flight International 13th, Power House, June, 2006
|
[49] |
Bewlay B P, Weimer M, Kelly T, Suzuki A, Subramanian P R. In: Baker I, Heilmaier M, Kuma S, Yoshimi K eds., Intermetallic-Based Alloys—Science, Technology and Applications, Materials Research Society Symposia Procedings, Vol.1516, Warrendale, PA: MRS, 2013: 49
|
[50] |
McQuay P. In: Kim Y W, Smarsly W, Lin J P, Dimiduk D eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2014: in
|
[51] |
Javis D J, Voss D. Mater Sci Eng, 2005; A413-414: 583
|
[52] |
Heppener M, Minster O, Jarvis D J. Acta Astronaut, 2008; 63: 20
|
[53] |
European Space Agency. Final Report of IMPRESS Project: Publishable Executive Summary, 2009: 1
|
[54] |
Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 1
|
[55] |
Kim Y W, Clemens H, Rosenberger A H eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2003: 1
|
[56] |
Kim Y W, Morris D, Yang R, Leyens C eds., Structural Aluminides for Elevated Temperatures, Warrendale, PA: TMS, 2008: 1
|
[57] |
Kim Y W, Smarsly W, Lin J P, Dimikuk D eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2014: 1
|
[58] |
Hanamura T, Uemori R, Tanino M. J Mater Res, 1988; 3: 656
|
[59] |
Huang S C, Hall E L. Metall Trans, 1991; 22A: 2619
|
[60] |
Kawabata T, Tamura T, Izumi O. Metall Trans, 1993; 24A: 141
|
[61] |
Sun F S, Cao C X, Kim S E, Lee Y T, Yan M G. Metall Mater Trans, 2001; 32A: 1573
|
[62] |
Beddoes J, Seo D Y, Chen W R, Zhao L. Intermetallics, 2001; 9: 915
|
[63] |
Huang Z W, Voice W, Bowen P. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermallics, Warrendale, PA: TMS, 2001: 551
|
[64] |
Stark A, Oehring M, Pyczak F, Schrreyer A. Adv Eng Mater, 2011; 13: 700
|
[65] |
Yu R, He L L, Cheng Z Y, Zhu J, Ye H Q. Intermetallics, 2002; 10: 661
|
[66] |
Paul J D H, Appel F, Wagner R. Acta Mater, 1998; 46: 1075
|
[67] |
Zhang W J, Deevi S C, Chen G L. Intermetallics, 2002; 10: 403
|
[68] |
Fröbel U, Appel F. Acta Mater, 2002; 50: 3693
|
[69] |
Woodward C, Kajihara S A, Rao S I, Dimiduk D M. In: George E P, Mills M J, Yamaguchi M eds., High-Temperature Ordered Intermetallic Alloys VIII. Warrendale, PA: MRS, 1999: KK281
|
[70] |
Li Y J, Hu Q M, Xu D S, Yang R. Intermetallics, 2011; 19: 793
|
[71] |
Hao Y L, Xu D S, Cui Y Y, Yang R, Li D. Acta Mater, 1999; 47: 1129
|
[72] |
Yang R. In: Kim Y W, Smarsly W, Lin J P, Dimiduk D eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2014: 123
|
[73] |
Bryant J D, Christodoulou L, Maisano J R. Scr Metall Mater, 1990; 24: 33
|
[74] |
Cheng T T. Intermetallics, 2000; 8: 29
|
[75] |
Hu D. Intermetallics, 2001; 9: 1037
|
[76] |
Hecht U, Witusiewicz V, Drevermann A, Zollinger J. Intermeta-llics, 2008; 16: 969
|
[77] |
Kitkamthorn U, Zhang L C, Aindow M. Intermetallics, 2006; 14: 759
|
[78] |
Lindemann J, Glavatskikh M, Leyens C, Ross-Fagaraseanu D. In: Kim Y W, Morris D, Yang R, Leyens C eds., Structural Aluminides for Elevated Temperatures, Warrendale, PA: TMS, 2008: 257
|
[79] |
Chen S, Beaven P A, Wagner R. Scr Metall Mater, 1992; 26: 1205
|
[80] |
Tian W H, Sano T, Nemoto M. Philos Mag, 1993; 68A: 965
|
[81] |
Appel F, Fischer F D, Clemens H. Acta Mater, 2007; 55: 4915
|
[82] |
Tsuyama S, Mitao S, Minakawa K N. Mater Sci Eng, 1992; A153: 451
|
[83] |
Noda T, Okabe M, Isobe S, Sayashi M. Mater Sci Eng, 1995; A192-193: 774
|
[84] |
Yu R, He L L, Guo J T, Ye H Q, Lupinc V. Acta Mater, 2000; 48: 3701
|
[85] |
Huguet A, Menand A. Appl Surf Sci, 1994; 76-77: 191
|
[86] |
Neroc-Partaix A, Menand A. Scr Mater, 1996; 35: 199
|
[87] |
Kawabata T, Tadano M, Izumi O. Scr Metall, 1988; 22: 1725
|
[88] |
Kawabata T, Abumiya T, Izumi O. Acta Metall Mater, 1992; 40: 2557
|
[89] |
Ponchel A. PhD Dissertation, Universite Pierre et Marie Curie Paris VI, 2001
|
[90] |
Thomas M, Bacos M P. Aerosp Lab, 2011; 3: 1
|
[91] |
Grange M, Raiart J L, Thomas M. Metall Mater Trans, 2004; 35A: 2087
|
[92] |
Clemens D R. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structrual Intermetallics 2001, Warrendale, PA: TMS, 2001: 217
|
[93] |
De Graef M, Biery N, Rishel L, Pollock T M, Cramb A. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 247
|
[94] |
Johnson D R, Inui H, Yamaguchi M. Intermetallics, 1998; 6: 647
|
[95] |
Küstner V, Oehring M, Chatterjee A, Güther V, Brokmeier H G, Clemens H, Appel F. In: Kim Y W, Clemens H, Rosenberger A H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 2003: 89
|
[96] |
Hecht U, Daloz D, Lapin J, Drevermann A, Witusiewicz V T, Zollinger J. In: Palm M, Bewlay P B, He Y H, Takeyama M, Wiezorek J M K eds., Mater Research Society Symposium Proceedings, Warrendale, PA: MRS, 2009: paper No.1128-U03-01
|
[97] |
Jung J Y, Park J K, Chun C H. Intermetallics, 1999; 7: 1033
|
[98] |
Eiken J, Appel M, Witsuiewicz V T, Zollinger J, Hecht U. J Phys Condens Matter, 2009; 21: 464104
|
[99] |
Kim J H, Shin D H, Semiatin S L, Lee C S. Mater Sci Eng, 2003; A344: 146
|
[100] |
Seetharaman V, Semiatin S L. Metall Mater Trans, 2002; 33A: 3817
|
[101] |
Cahn R W, Takeyama M, Horton J A, Liu C T. J Mater Res, 1991; 6: 57
|
[102] |
Yang R, Botton G A, Cahn R W. Acta Mater, 1996; 44: 3869
|
[103] |
Semiatin S L, Chesnutt J C, Austin C, Seetharaman V. In: Nathal M V, Darolia R, Liu C T, Martin P L, Miracle D B, Wagner R, Yamaguchi M eds., Structural Intermetallics, Warrendale, PA: TMS, 1997: 263
|
[104] |
Fukutomi H, Nomoto A, Osuga Y, Ikeda S, Mecking H. Intermetallics, 1996; 4: S49
|
[105] |
Salishchev G A, Imayev R M, Senkov O N, Imayev V M, Gabdullin N K, Shagiev M R, Kuznetsov A V, Froes F H. Mater Sci Eng, 2000; A286: 236
|
[106] |
Imayev R M, Salishchev G A, Imayev V M, Shagiev M R, Kuznetsov M R, Appel F, Oehring M, Senkov O N, Froes F H. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 565
|
[107] |
Imayev R M, Imayev V M, Oehring M, Appel F. Metall Mater Trans, 2005; 36A: 859
|
[108] |
Fröbel U, Appel F. Metall Mater Trans, 2007; 38A: 1817
|
[109] |
Sun W. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009
|
[109] |
(孙伟. 中国科学院金属研究所博士学位论文, 沈阳, 2009)
|
[110] |
Oehring M, Lorenz U, Niefanger R, Christoph U, Appe F, Wagner R, Clemens H, Eberhardt N. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 439
|
[111] |
Oehring M, Lorenz U, Appel F, Roth-Fagaraseanu D. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics, Warrendale, PA: TMS, 2001: 157
|
[112] |
Liu R C, Liu D, Tan J, Cui Y Y, Yang R, Liu F Y, Withey P A. Intermetallics, 2014; 52: 110
|
[113] |
Doherty R D, Hughes D A, Humphreys F J, Jonas J J, Jensen D J, Kassner M E, King W E, McNelley T R, McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238: 219
|
[114] |
Brokmeier H G, Oehring M, Lorenz U, Clemens H, Appel F. Metall Mater Trans, 2004; 35A: 3563
|
[115] |
Zhang W J, Deevi S C. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics, Warrendale, PA: TMS, 2001: 699
|
[116] |
Veyssière P. Mater Sci Eng, 2001; A309-310: 44
|
[117] |
Es-Souni M, Bartels A, Wagner R. Mater Sci Eng, 1995; A192-193: 698
|
[118] |
Worth D B, Jones J W, Allison J E. Metall Trans, 1995; 26A: 2947
|
[119] |
Morris M A, Leboeuf T. Intermetallics, 1997; 5: 339
|
[120] |
Wang J G, Hsiung L M, Nieh T G. Scr Mater, 1998; 39: 957
|
[121] |
Maruyama K, Yamamoto R, Nakakuki H, Fujitsuna N. Mater Sci Eng, 1997; A239-240: 419
|
[122] |
Parthasarathy T A, Subramanian P R, Mendiratta M G, Dimiduk D M. Acta Mater, 2000; 48: 541
|
[123] |
Hayes R W, Martin P L. Acta Metall Mater, 1995; 43: 2761
|
[124] |
Zhang W J, Spigarelli S, Cerri E, Evangelista E, Francesconi L. Mater Sci Eng, 1996; A211: 15
|
[125] |
Du X W, Zhu J, Kim Y W. Intermetallics, 2001; 9: 137
|
[126] |
Appel F. Intermetallics, 2001; 9: 907
|
[127] |
Es-Souni M, Bartels A, Wagner R. Acta Metall Mater, 1995; 43: 153
|
[128] |
Zhang W J, Deevi S C. Intermetallics, 2003; 11: 177
|
[129] |
Taniguchi S, Hongawara N, Shibata T. Mater Sci Eng, 2001; A307: 107
|
[130] |
Brady M P, Smialek J L, Humphrey D L, Smith J. Acta Mater, 1997; 45: 2371
|
[131] |
Zeller A, Dettenwanger F, Schütze M. Intermetallics, 2002; 10: 59
|
[132] |
Rahmel A, Quadakkers W J, Schütze M. Mater Corros, 1995; 46: 271
|
[133] |
Quadakkers W J, Schaaf P, Zheng N, Gil A, Wallura E. Mater Corros, 1997; 48: 28
|
[134] |
Zhu L G, Hu Q M, Yang R, Ackland G J. J Phys Chem, 2012; 116C: 24201
|
[135] |
Schmiedgen M, Graat P C J, Baretzky B, Mittemeijer E J. Thin Solid Films, 2002; 415: 114
|
[136] |
Song Y, Dai J H, Yang R. Surf Sci, 2012; 606: 852
|
[137] |
Song Y, Xing F J, Dai J H, Yang R. Intermetallics, 2014; 49: 1
|
[138] |
Lang C, Schutze M. Oxid Met, 1996; 46: 284
|
[139] |
Ping F P, Hu Q M, Yang R. Acta Metall Sin, 2013; 49: 385
|
[139] |
(平发平, 胡青苗, 杨锐. 金属学报, 2013; 49: 385)
|
[140] |
Li X Y, Taniguchi S. Intermetallics, 2004; 12: 11
|
[141] |
Kumagai M, Shibue K, Kim M S, Furuyama T. US Pat, 5,451,366., 1995
|
[142] |
Masset P J, Neve S, Zschau H E, Schütze M. Mater Corros, 2008; 59: 609
|
[143] |
Deve H E, Evans A G. Acta Metall Mater, 1991; 39: 1171
|
[144] |
Mitao S, Tsuyama S, Minakawa K. Mater Sci Eng, 1991; A143: 51
|
[145] |
Chan K S, Kim Y W. Acta Metall Mater, 1995; 43: 439
|
[146] |
Song Y, Xu D S, Yang R, Li D, Hu Z Q. Intermetallics, 1998; 6: 157
|
[147] |
Song Y, Yang R, Li D, Hu Z Q, Guo Z X. Intermetallics, 2000; 8: 563
|
[148] |
Song Y, Guo Z X, Yang R, Li D. Comput Mater Sci, 2002; 23: 55
|
[149] |
Yoo M H, Fu C L. Mater Sci Eng, 1992; A153: 470
|
[150] |
Yoo M H, Zou J, Fu C L. Mater Sci Eng, 1995; A192-193: 14
|
[151] |
Nakano T, Kawanaka T, Yasuda H Y, Umakoshi Y. Mater Sci Eng, 1995; A194: 43
|
[152] |
Yokoshima S, Yamaguchi M. Acta Mater, 1996; 44: 873
|
[153] |
Appel F. Philos Mag, 2005; 85: 205
|
[154] |
Lorenz U, Appel F, Wagner R. Mater Sci Eng, 1997; A234-236: 846
|
[155] |
Sastry S M L, Lipsitt H A. Metall Trans, 1977; 8A: 299
|
[156] |
Larsen J M. In: Kim Y W, Dimiduck D M, Loretto M eds., Gamma Titanium Aluminides, Warrendal, PA: TMS, 1999: 463
|
[157] |
Vaidya W V, Schwalbe K H, Wagner R. In: Kim Y W, Wagner R, Yamaguchi M eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1995: 867
|
[158] |
Trail S J, Bowen P. Mater Sci Eng, 1995; A193: 427
|
[159] |
Harding T S, Jones J W. Scr Mater, 2000; 43: 623
|
[160] |
Draper S L, Lerch B A, Pereira J M, Nathal M V, Nazmy M Y, Staubli M. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics, Warrendale, PA: TMS, 2001: 295
|
[161] |
Harding T S, Jones J W. Metall Mater Trans, 2001; 32A: 2975
|
[162] |
Umakoshi Y, Yasuda H Y, Nakano T. Intermetallics, 1996; 4: S65
|
[163] |
Recina V. Mater Sci Technol, 2000; 16: 333
|
[164] |
Gloanec A L, Bertheau D, Jouiad M, Henaff G, Grange M, Belaygue P. In: Kim Y W, Rosenberger A H, Clemens H eds., Gamma Titanium Aluminides, San Diego, CA: TMS, 2003: 485
|
[165] |
Park Y S, Nam S W, Hwang S K. Mater Lett, 2002; 53: 392
|
[166] |
Appel F, Heckel T K, Christ H J. Int J Fatigue, 2010; 32: 792
|
[167] |
Hénaff G, Gloanec A L. Intermetallics, 2005; 13: 543
|
[168] |
Hénaff G, Tonneau A, Mabru C. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics 2001, Warrendale, PA: TMS, 2001: 571
|
[169] |
Kruzic J J, Campbell J P, McKelvey A L, Choe H, Ritchi R O. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 495
|
[170] |
Campbell J P, Kruzic J J, Lillibridge S, Venkateswara Rao K T, Ritchie R O. Scr Mater, 1997; 37: 707
|
[171] |
McQuay P A, Sikka V K. In: Westbrook J H, Fleischer R L eds., Intermetallic Compounds—Principles and Practice. Vol.3, London: Wiley, 2002: 591
|
[172] |
Harding R A, Wickins M, Wang H, Djambazov G, Pericleous K A. Intermetallics, 2011; 19: 805
|
[173] |
Aguilar J, Schievenbusch A, Kättlitz O. Intermetallics, 2011; 19: 757
|
[174] |
Oehring M, Appel F, Paul J D H, Imayev R M, Imaye V M, Lorenz U. Mater Sci Forum, 2010; 638-642: 1394
|
[175] |
Hu D, Jiang H, Wu X. Intermetallics, 2009; 17: 744
|
[176] |
Imayev R M, Imayev V M, Oehring M, Appel F. Intermetallics, 2007; 15: 451
|
[177] |
Thomas M, Raviart J L, Popoff F. Intermetallics, 2005; 13: 944
|
[178] |
Clemens H, Kestler H, Eberhardt N, Knabl W. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 209
|
[179] |
Gerling R, Clemens H, Schimansky F P. Adv Eng Mater, 2004; 6: 23
|
[180] |
Graves J A, Perepezko J H, Ward C H, Froes F H. Scr Metall, 1987; 21: 567
|
[181] |
Huang A, Hu D, Loretto M H, Mei J, Wu X. Scr Mater, 2007; 56: 253
|
[182] |
Xu L, Bai C G, Liu D, Sun W, Yu D J, Cui Y Y, Yang R. In: Kim Y W, Morris D, Yang R, Leyens C eds., Structural Aluminides for Elevated Temperatures, Warrendale, PA: TMS, 2008: 179
|
[183] |
Xu L, Wu J, Cui Y Y, Yang R. In: Kim Y W, Smarsly W, Lin J P, Dimiduk D eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2014: 195
|
[184] |
Integrated Computational Materials Engineering (ICME). Implementing ICME in the Aerospace, Automotive and Maritime Industries. Warrendale, PA: TMS, 2013: 1
|
[185] |
Lasalmonie A. Intermetallics, 2006; 14: 1123
|
[186] |
Inui H, Oh M H, Nakamura A, Yamaguchi M. Acta Metall Mater, 1992; 40: 3095
|
[187] |
Yokoshima S, Yamaguchi M. Acta Mater, 1996; 44: 873
|
[188] |
Jin H, Liu R H, Cui Y Y, Xian Q G, Xu D S, Yang R. In: Kim Y W, Smarsly W, Lin J P, Dimiduk D eds., Gamma Titanium Aluminide, Warrendale, PA: TMS, 2014: 143
|
[189] |
Couret A, Molenat G, Galy J, Thomas M. Intermetallics, 2008; 16: 1134
|
[190] |
Moll J H, Whitney E, Yolton C F, Habel U. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 255
|
[191] |
Srivastava D, Chang I T H, Loretto M H. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 265
|
[192] |
Murr L E, Gaytan S M, Ceylan A, Martinez E, Martinez J L, Hernandez D H, Bachado B I, Ramirez D A, Medina F, Collins S, Wicker R B. Acta Mater, 2010; 58: 1887
|
[193] |
Porter J, Wooten J, Harrysson O, Knowlson K. Materials Science and Technology—Association for Iron & Steel Technology. Vol.2, Warrendal, PA: Association for Iron & Steel Technology, 2011: 1434
|
[194] |
Franzén S F, Karlsson J. Diploma Work No.37/2010, Chalmers University of Technology, Sweden, 2010
|
[195] |
Terner M, Biamino S, Epicoco P, Penna A, Hedin O, Sabbadini S, Fino P, Pavese M, Ackelid U, Gennaro P, Pelissero F, Badni C. Steel Res Int, 2012; 83: 943
|
[196] |
Biamino S, Klöden B, Weissgärber T, Kieback B, Ackelid U. Franuhofer Direct Digital Manufacturing Conference, Berlin, Germany: DDMC, 2014: 1
|
[197] |
Leyens C, Frückner F, Nowotny S. Presented at TMS Symposium on Gamma Titanium Aluminide, 16-20 February 2014, San Diego, USA
|
[198] |
Jüchter V, Schwerdtfeger J, Körner C. Presented at TMS Symposium on Gamma Titanium Aluminide, 16-20 February 2014, San Diego, USA
|
[199] |
European Science Foundation, Materials ScienceEngineering Expert Committee (MatSEEC). Materials Science and Engineering in Europe: Challengers and Opportunities. Science Position Paper, November, 2013
|
[200] |
Gartner′s 2012 Hype Cycle for Emerging Technologies Identifies ‘Tipping Point’ Technologies That Will Unlock Long-Awaited Technology Scenarios. artner′s 2012 Hype Cycle for Emerging Technologies Identifies ‘Tipping Point’ Technologies That Will Unlock Long-Awaited Technology Scenarios. (accessed 2014.06.10
|
[201] |
Harrop J. Application of 3D Printing 2014-2024: Forcasts, Markets, Players. IDTechEx Report, 2014
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|